Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.05 kN/m | 6.00 pli | at elevated temperature; IPC-TM-650.2.4.8.2a |
Park Electrochemical Nelco® N7000-1 Polyimide Laminate and Prepreg The Nelco N7000-1 series of polyimide laminate and prepreg has alow Z-axis expansion and high Tg offering PCB manufacturers consistent board performance and reliability. N7000-1 is a good choice for.. |
|||
Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
Arlon 19576R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat.. |
|||
Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
Arlon 55606R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, etched |
3M Scotchcal™ 8000-12 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, anodized |
3M Scotchcal™ 8000-13 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, etched |
3M Scotchcal™ 8000-23 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, etched |
3M Scotchcal™ 8000LF-10 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum |
3M Scotchlite™ 680-64 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum |
3M Scotchlite™ 680-71 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum |
3M Scotchlite™ 680-75 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum |
3M Scotchlite™ 680-85 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 32580X030 0.030" (0.762 mm) Uncured Unsupported Silicone Rubber on a PET Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Gray silicone gum on polymer linerThis data represents typical values for the production material. The data .. |
|||
Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
Arlon 41580R030 0.030" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
Arlon 41600R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
Arlon 49090R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass fabricThis data Represents typical values for the production material. The data should not be used to wr.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7909 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
Arlon R33468A030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured LayersAppearance: Semi-cured blue silicone gum on glass fabricThis data Represents typical values for the production material. .. |
|||
Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
Arlon R34369R028 0.029" (0.737 mm) Uncured Layer on Top of a Cured Layer on One Side with Fiberglass Substrate, 38" wide Design/Construction:Side 1: Uncured Layer on Top of a Cured Layer on One SideThis data Represents typical values for the production material. The data should not be used to write, or in place of, ma.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Bond Strength(S1 to S2); SQA-TMS-011 |
Arlon R35798R013 0.013" (0.330 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 Fiberglass Side 2: Uncured Silicone RubberThis data represents typic.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, etched |
3M Scotchcal™ 8000LF-23 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum |
3M Scotchlite™ 680-76 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Peel Strength | 1.05 kN/m | 6.00 pli | on canvas |
3M Scotch-Weld™ 3750LM Low Melt Adhesive Excellent "hot tack", fast setting for corrugated, beadboard, repack, recoup and Economical, general purpose and Use with AE II LET applicator onlyInformation provided by 3M |
|||
Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
Arlon 41580R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
Arlon 30600R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis da.. |