Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.912 kN/m | 5.20 pli | at elevated temperature; IPC-TM-650.2.4.8.2a |
Park Electrochemical Nelco® N7000-2 V0 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 V0 series is a next-generation high-Tg polyimide using a toughened resin chemistry to achieve a UL 94-V0 designation. This advanced material is designed for use in a wide variety o.. |
|||
Peel Strength | 0.912 kN/m | 5.20 pli | PVC vs. PVC, 24 minutes |
Taiwan PU Corporation TPUA-1560 TPU Shoe Adhesive A PU resin for general application with excellent adhesion to all kinds of media.Features: Fast crystallization rateGood initial adhesionGood thermo toleranceCan be used alone or combined with a cro.. |
|||
Peel Strength | 0.912 kN/m | 5.20 pli | PVC vs. PVC, 24 minutes |
Taiwan PU Corporation TPUA-760 TPU Shoe Adhesive A PU resin for general application with excellent adhesion to all kinds of media.Features: Fast crystallization rateGood initial adhesionGood thermo toleranceCan be used alone or combined with a cro.. |
|||
Peel Strength | 0.912 kN/m | 5.20 pli | To Kapton, After Solder |
Arlon 38N High Performance Polyimide Low-Flow 38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow.. |
|||
Peel Strength | 0.912 kN/m | 5.20 pli | Adhesion to Aluminum, etched |
3M Controltac™ 8620 ES Conformable Graphic Film These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Peel Strength | 0.912 kN/m | 5.20 pli | Adhesion to Aluminum, etched |
3M Controltac™ 8620Cv2 ES Changeable Graphic Film with Comply™ v2 Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Peel Strength | 0.912 kN/m | 5.20 pli | Polycarbonate, 180°, after 48 hrs at 23°C |
3M Fastbond™ 49 Insulation Adhesive 3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and .. |
|||
Peel Strength | 0.912 kN/m | 5.20 pli | Very smooth, tight polyester fabric, 180° |
3M Scotch-Weld™ 6116 Bulk only Adhesive Same as 6111 but Lower than normal viscosity and mainly used on fabrics.Information provided by 3M |
|||
Peel Strength | 0.912 kN/m | 5.20 pli | Adhesion to Aluminum, etched |
3M Controltac™ 8620Cv3 ES Changeable Graphic Film with Comply™ v3 Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Peel Strength | 0.912 kN/m | 5.20 pli | Adhesion to Aluminum, etched |
3M Controltac™ 8620C ES Changeable Graphic Film with Comply™ Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Peel Strength | 0.912 kN/m | 5.20 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 44141R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent.. |