Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | >= 3.51 kN/m | >= 20.0 pli | steel/steel |
Resinlab® AR 4315 Metal Bonding Methacrylate Adhesive Resinlab™ AR 4315 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any .. |
|||
Peel Strength | 3.51 - 4.38 kN/m | 20.0 - 25.0 pli | |
ITW Devcon 10 minuteâ„¢ Epoxy, Black Information provided by ITW Devcon |
|||
Peel Strength | 3.51 - 4.73 kN/m | 20.0 - 27.0 pli | |
ITW Devcon Flex Welderâ„¢ Methacrylate Adhesive FC, Off-White, Black Information provided by ITW Devcon |
|||
Peel Strength | 3.51 - 4.73 kN/m | 20.0 - 27.0 pli | |
ITW Devcon Flex Welderâ„¢ Methacrylate Adhesive, Off-White Information provided by ITW Devcon |
|||
Peel Strength | >= 3.51 kN/m | >= 20.0 pli | |
Master Bond EP21TDCHT-LO Room Temperature Curing, Toughened Two Component Epoxy Master Bond Polymer Adhesive EP21TDCHT-LO is a two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a very forgiving and convenient one .. |
|||
Peel Strength | >= 3.51 kN/m | >= 20.0 pli | |
Master Bond EP21TDCNFL Two Component Nickel Conductive Epoxy Adhesive Master Bond Polymer System EP21TDCNFL is a two component, nickel filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl.. |
|||
Peel Strength | >= 3.51 kN/m | >= 20.0 pli | |
Master Bond EP21TDCSFL Flexible Two Component Silver Conductive Epoxy Master Bond Polymer System EP21TDCSFL is a two component, silver filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl.. |
|||
Peel Strength | >= 3.51 kN/m | >= 20.0 pli | Al/Al |
Master Bond Supreme 3HTND-1SM Fast Curing, One Component, Surface Mount Adhesive Master Bond Polymer System Supreme 3HTND-1SM is a one component, exceptionally fast curing surface mount adhesive system with exceptional toughness and durability. It has high shear and peel strengt.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | |
Tra-Con Tra-Bond 724-14C Polyurethane Adhesive TRA-BOND 724-14C premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong, resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar.. |
|||
Peel Strength | 3.51 kN/m @Temperature 82.2 °C |
20.0 pli @Temperature 180 °F |
T-Peel, 2 hrs @ 250°F, Metal Clamp Pressure, 6061 T6 FPL Etched |
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhe.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | |
Dow Corning 786 SILICONE MILDEW RESISTANT SEALANT Dow Corning® 786 Silicone Sealant is designed to seal nonporous surfaces around showers, tubs, sinks and plumbing fixtures where conditions of high humidity and temperature extremes exist.Informati.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | T-Peel |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Peel Strength | 3.51 kN/m @Temperature -55.0 °C |
20.0 pli @Temperature -67.0 °F |
Bell Pell Adhesion, Aluminum Etched, Cohesive Failure; ASTM D3167 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | PVC, Hi-Impact, 180° after aging 1-2 days @ RT and 1 day |
3M Scotch-Weld™ Hi-Strength Postforming 4693 High Performance Industrial Plastic Adhesives Features:Low viscosity grade for spray or brush applicationClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstanding bond strengt.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | ABS, 180° after aging 1-2 days @ RT and 1 day |
3M Scotch-Weld™ Hi-Strength Postforming 4693H High Performance Industrial Plastic Adhesives Features: High Viscosity grade in collapsible tubes for flow applicationsClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstandin.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | PVC, Hi-Impact, 180° after aging 1-2 days @ RT and 1 day |
3M Scotch-Weld™ Hi-Strength Postforming 4693H High Performance Industrial Plastic Adhesives Features: High Viscosity grade in collapsible tubes for flow applicationsClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstandin.. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | Steel-Unsupported Vinyl, 180°, Aging 7 Day @ 140°F |
3M Scotch-Weld™ 2262 Plastic Adhesive Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very .. |
|||
Peel Strength | 3.51 kN/m | 20.0 pli | on canvas |
3M Scotch-Weld™ 3747 Hot Melt Adhesive General purpose for wide variety of plastics, wood and lightweight metalsInformation provided by 3M |
|||
Peel Strength | 3.51 kN/m @Temperature 82.0 °C |
20.0 pli @Temperature 180 °F |
Aluminum, T-Peel |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Peel Strength | 3.51 - 12.3 kN/m | 20.0 - 70.0 pli | Varies with substrates. |
Loctite® Durabond® E-60HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |