Information provided by ITW Devcon
Physical Properties Metric English Comments
Viscosity 52000 cP
52000 cP
Mixed Viscosity
Mechanical Properties Metric English Comments
Elongation at Break 120 %
120 %
Adhesive Bond Strength 10.3 MPa
1500 psi
lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002
Tensile Impact Strength 42.0 kJ/m²
20.0 ft-lb/in²
Peel Strength 3.51 - 4.73 kN/m
20.0 - 27.0 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
dry
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
dry
Processing Properties Metric English Comments
Cure Time 9.00 - 12.0 min
0.150 - 0.200 hour
Working time
40.0 - 45.0 min
0.667 - 0.750 hour
Fixture time
120 - 240 min
2.00 - 4.00 hour
Functional cure
Descriptive Properties Value Comments
Mix ratio (Resin:Hardener) 1:1