Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.09861 kN/m | 0.5625 pli | Adhesion to Steel; ASTM D3330 |
3M 24S56W Automotive Protective Tape 3M™ Automotive Protective Tape 24S56W has a medium-tack adhesive system to help provide temporary protection for many painted metal finishes and plastics with minimum adhesion build-up for clean re.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | Adhesion to Steel; ASTM D3330 |
3M 25A26 Co-Extruded Polyethylene Protective Tapes 3M™ Co-Extruded Polyethylene Protective Tape helps provide temporary protection of painted metals, glass and plastics from surface damage, such as scratching, abrading. etc.Information provided by .. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | Adhesion to Steel; ASTM D3330 |
3M 25A29 Co-Extruded Polyethylene Protective Tapes 3M™ Co-Extruded Polyethylene Protective Tape helps provide temporary protection of painted metals, glass and plastics from surface damage, such as scratching, abrading. etc.Information provided by .. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | Adhesion to Steel; ASTM D3330 |
3M 31U72C (Clear) Polyethylene Protective UV Tape 3M™ Protective UV Tape 31U72C is a 3 mil clear polyethylene self-wound film coated with a medium-high tack adhesive system featuring UV resistance.Information provided by 3M |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | Adhesion to Steel; ASTM D3330 |
3M 3294 Vent Tape 3M™ Vent Tape 394 is a non-woven, synthetic backing with a strip-coated low-tack pressure sensitive adhesive for use in various venting applications requiring high outgassing rates.Information prov.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | Adhesion to Steel; ASTM D3330 |
3M 44S56W Automotive Protective Tape 3M™ Automotive Protective Tape 44S56W has a medium-tack adhesive system to help provide temporary protection for many painted metal finishes and plastics with minimum adhesion build-up for clean re.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7745FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Film 7745FL utilizes a matte clear polyester that is recommended for optimum durability and appearance in dot matrix and hand writable applications. The matte coating r.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | Polypropylene, 90° peel, 12"/min, 72 hr dwell RT; ASTM D3330 |
3M 9447 Adhesive Transfer Tape 3M™ Adhesive Transfer Tape 9447 is specifically designed for use with 3M™ Label Component Systems for protected graphics printing of polyester films. Also can be used in constructing custom tamper.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7011 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7880 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Material 7880 is a 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for traditional.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7880HL Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 78 lb clay-coated kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abras.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7883HL Computer-Imprintable Polyester Label Material Information provided by 3M |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7893 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7920 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7920 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. 3M™ Adhesive .. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7924 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7931 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7950 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7983 Sheet Polyester Label Material Features:Matte coating is compatible with screen printing and resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations. Variable information can be added by the end .. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7776 Polypropylene Label Material 3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adh.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7884 White Vinyl Label Material Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and.. |
|||
Peel Strength | 0.09861 kN/m | 0.5625 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7887 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |