Material Notes:
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmness and strength on a variety of surfaces including high surface energy (HSE) and low surface energy (LSE) plastics, as well as, metals.Information provided by 3M
Physical Properties Metric English Comments
Thickness 22.9 microns
0.900 mil
Adhesive
63.5 microns
2.50 mil
Facestock
63.5 microns
2.50 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.09861 kN/m
0.5625 pli
Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
0.110 kN/m
0.625 pli
HD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
0.1205 kN/m
0.6875 pli
LD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
0.1205 kN/m
0.6875 pli
LD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.1424 kN/m
0.8125 pli
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.175 kN/m
1.00 pli
HD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.23008 kN/m
1.3125 pli
Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.23008 kN/m
1.3125 pli
HD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.2849 kN/m
1.625 pli
LD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.307 kN/m
1.75 pli
LD Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.31773 kN/m
1.8125 pli
LD Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
0.351 kN/m
2.00 pli
HD Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
0.3725 kN/m
2.125 pli
HD Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.3725 kN/m
2.125 pli
HD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.42729 kN/m
2.4375 pli
LD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.51494 kN/m
2.9375 pli
Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
0.570 kN/m
3.25 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
50.0 °C
122 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 320 Acrylic
Liner 43# Densified Kraft