Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 10.5 - 11.4 kN/m | 60.0 - 65.0 pli | |
ITW Devcon Composite Welderâ„¢ Methacrylate Adhesive FS, Blue Green, Black Information provided by ITW Devcon |
|||
Peel Strength | 10.5 kN/m | 60.0 pli | At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle |
Momentive Performance Materials RTV142 White, Low Volatile, One Component Silicone Sealant RTV 142 one-component, ready-to-use adhesive sealant cures to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Methyl alcohol vapors are released.. |
|||
Peel Strength | 10.5 kN/m | 60.0 pli | Cured 7 days at 25°C and 50% relative humidity |
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray RTV 157 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15.. |
|||
Peel Strength | 10.5 kN/m | 60.0 pli | Cured 7 days at 25°C and 50% relative humidity |
Momentive Performance Materials RTV159 High Strength Silicone Adhesive Sealant, Red RTV 159 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15.. |
|||
Peel Strength | 10.5 kN/m | 60.0 pli | T-Peel, Etched Aluminum, 17-20 mil bondline |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Peel Strength | 10.5 kN/m @Temperature 23.0 °C |
60.0 pli @Temperature 73.4 °F |
Aluminum, T-Peel |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Peel Strength | 10.5 kN/m | 60.0 pli | Bell Peel Adhesion, Aluminum-etched, Cohesive Failure; ASTM D3167 |
3M Scotch-Weld™ LSB90 Flexible Epoxy 3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife.. |
|||
Peel Strength | 10.5 kN/m | 60.0 pli | 180°, Polycarbonate |
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 10.5 kN/m | 60.0 pli | 180°, Glass |
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |
|||
Peel Strength | 10.5 kN/m | 60.0 pli | Aluminum Etched, T-Peel, 17-20 mil bondline |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |