Mechanical Properties Metric English Comments
Peel Strength 0.69024 kN/m
3.9375 pli
Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7779 Polypropylene Label Material
3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating..
Peel Strength 0.69024 kN/m
3.9375 pli
Smooth Powder Coating, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7779 Polypropylene Label Material
3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating..
Peel Strength 0.69024 kN/m
3.9375 pli
polycarbonate, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
3M 9502 Adhesive Transfer Tapes with Adhesive 220
3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p..
Peel Strength 0.69024 kN/m
3.9375 pli
polycarbonate, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
3M 9505 Adhesive Transfer Tapes with Adhesive 220
3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p..
Peel Strength 0.69024 kN/m
3.9375 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7903 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 0.69024 kN/m
3.9375 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7903FL Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 0.69024 kN/m
3.9375 pli
Smooth Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7904 Screen Printable Sheet Vinyl Label Material
3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili..
Peel Strength 0.69024 kN/m
3.9375 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7904 Screen Printable Sheet Vinyl Label Material
3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili..
Peel Strength 0.69024 kN/m
3.9375 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7905 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 0.69024 kN/m
3.9375 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7907 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat..
Peel Strength 0.69024 kN/m
3.9375 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7908 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 0.69024 kN/m
3.9375 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7908FL Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 0.69024 kN/m
3.9375 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7909 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 0.69024 kN/m
3.9375 pli
90° Peel, PET/PET, 72 hrs at RT; ASTM D3330
3M 7995MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Peel Strength 0.69024 kN/m
3.9375 pli
polycarbonate, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
3M 9552 Adhesive Transfer Tapes with Adhesive 220
3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p..
Peel Strength 0.69024 kN/m
3.9375 pli
polycarbonate, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
3M 9555 Adhesive Transfer Tapes with Adhesive 220
3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p..