3M 9552 Adhesive Transfer Tapes with Adhesive 220

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 9552 Adhesive Transfer Tapes with Adhesive 220.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information provided by 3M
Physical Properties Metric English Comments
Thickness 58.4 microns
2.30 mil
Mechanical Properties Metric English Comments
Peel Strength 0.438 kN/m
2.50 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 15 min at RT, 2.3 mil; ASTM D3330
0.58068 kN/m
3.3125 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 15 min at RT, 4.9 mil; ASTM D3330
0.60259 kN/m
3.4375 pli
ABS, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330
0.60259 kN/m
3.4375 pli
polycarbonate, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330
0.69024 kN/m
3.9375 pli
polycarbonate, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
0.71216 kN/m
4.0625 pli
ABS, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
0.7669 kN/m
4.375 pli
glass, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330
0.8108 kN/m
4.625 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 2.3 mil; ASTM D3330
0.97511 kN/m
5.5625 pli
glass, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
1.074 kN/m
6.125 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
1.4353 kN/m
8.1875 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at 70°C, 2.3 mil; ASTM D3330
1.895 kN/m
10.81 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at 70°C, 4.9 mil; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Long term
177 °C
351 °F
Short term
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Adhesive Type 220
Liner Tan 58# Polycoated Kraft