Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.131 kN/m | 0.750 pli | Adhesion |
Dielectric Polymers NT-7411-5 Fume Mask
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Good conformabilityChemical resistantApplications: For protecting large areas of printed circuit boards from splash and fumes duri.. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | Adhesion to Steel; ASTM D3330 |
3M 394 Vent Tape 3M™ Vent Tape 394 is a non-woven, synthetic backing that meets most typical outgassing requirements for foam-in-place insulation processes in appliance and other industries and contains fungicide f.. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7600 Removable Vinyl Label Material 3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent.. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7600 Removable Vinyl Label Material 3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent.. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7744FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7745FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Film 7745FL utilizes a matte clear polyester that is recommended for optimum durability and appearance in dot matrix and hand writable applications. The matte coating r.. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7745FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Film 7745FL utilizes a matte clear polyester that is recommended for optimum durability and appearance in dot matrix and hand writable applications. The matte coating r.. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | Steel, 180° Peel, 72 hr dwell, Backside; ASTM D3330 |
3M 9425 Repositionable Tape 3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | Steel, 180° Peel, 72 hr dwell, Backside; ASTM D3330 |
3M 9425HT Repositionable Tape 3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | Adhesion to Steel; ASTM D3330 |
3M 5401 Traction Tape 3M™ Traction Tape 5401 is a single coated glass cloth tape with silicone coated backing used for wrapping rollers to provide traction and non-stick surface.Information provided by 3M |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7845TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7845TL is a matte clear polyester designed for sheet fed laser imprinting. This label material utilizes 3M™ Adhesive 310 which provides firmness .. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7920 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7920 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. 3M™ Adhesive .. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | Linered side-Photopolymer, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1060 Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | Adhesion to Steel; ASTM D3330 |
3M 483 Polyethylene Tape 3M™ Polyethylene Tape 483 has a polyethylene backing with a rubber adhesive for many general purpose applications including sealing, color coding, protecting, moisture proofing. Black tape has exce.. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7744 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7744 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.131 kN/m | 0.750 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |