3M 9425 Repositionable Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 9425 Repositionable Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M
Physical Properties Metric English Comments
Thickness 35.6 microns
1.40 mil
Carrier
107 microns
4.20 mil
Liner
147 microns
5.80 mil
Tape
Mechanical Properties Metric English Comments
Peel Strength 0.131 kN/m
0.750 pli
Steel, 180° Peel, 72 hr dwell, Backside; ASTM D3330
0.49303 kN/m
2.8125 pli
Steel, 180° Peel, 72 hr dwell, Faceside; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 52.0 °C
126 °F
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Carrier UPVC
Adhesive Type Backside
Faceside
Appearance Clear
Liner 58# Natural Polycoated Kraft