3M 483 Polyethylene Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 483 Polyethylene Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Polyethylene Tape 483 has a polyethylene backing with a rubber adhesive for many general purpose applications including sealing, color coding, protecting, moisture proofing. Black tape has excellent UV resistance and can be used outdoors for up to 12 months.Information provided by 3M
Physical Properties Metric English Comments
Thickness 99.1 microns
3.90 mil
Backing; ASTM D3752
127 microns
5.00 mil
Total; ASTM D3752
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.5 MPa
1960 psi
ASTM D3759
Elongation at Break 300 %
300 %
ASTM D3759
Peel Strength 0.131 kN/m
0.750 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Transparent, red, blue, white, black, yellow