Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | >= 200 g/25 mm | >= 200 g/in | at 135°C, 15 psi pressure and 1 sec. |
Total PPR 7450HC Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor - Low catalyst residuals in FINA 7450HC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 7450HC improves its .. |
|||
Seal Strength | >= 200 g/25 mm | >= 200 g/in | at 135°C, 15 psi pressure and 1 sec. |
Total PPR 8573 Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8573 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The low m.. |
|||
Seal Strength | >= 200 g/25 mm | >= 200 g/in | at 135°C, 15 psi pressure and 1 sec. |
Total PPR 8473 Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8473 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The very .. |
|||
Seal Strength | 200 g/25 mm @Pressure 0.00345 MPa, Temperature 100 °C |
200 g/in @Pressure 0.500 psi, Temperature 212 °F |
LPS, 0.5 sec, Both Sides; ExxonMobl Method |
ExxonMobil Bicor™ 21MBT621 OPP Film Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both side. The static resistant feature of this film prevents the attraction of dust, and.. |
|||
Seal Strength | 200 g/25 mm @Pressure 0.00345 MPa, Temperature 105 °C |
200 g/in @Pressure 0.500 psi, Temperature 221 °F |
LSP, 0.5 sec; ExxonMobil Method |
ExxonMobil Bicor™ 25MBT666 OPP Film Product Description: Biaxially oriented polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping offering unique aspect and cost reduction advant.. |
|||
Seal Strength | 200 g/25 mm @Pressure 0.00345 MPa, Temperature 100 °C |
200 g/in @Pressure 0.500 psi, Temperature 212 °F |
0.5 sec; ExxonMobil Method |
ExxonMobil Bicor™ 30MB666 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, .. |
|||
Seal Strength | 200 g/25 mm @Pressure 0.00345 MPa, Temperature 100 °C |
200 g/in @Pressure 0.500 psi, Temperature 212 °F |
LPS, 0.5 sec; ExxonMobil Method |
ExxonMobil Bicor™ 30MBT666 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping, offering unique aspect and cost r.. |
|||
Seal Strength | 200 g/25 mm @Pressure 0.00345 MPa, Temperature 100 °C |
200 g/in @Pressure 0.500 psi, Temperature 212 °F |
0.5 sec, Untreated Surface; ExxonMobl Method |
ExxonMobil Bicor™ 20MBT666 OPP Film Product Description: Bicor 20MBT666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. This film is specifically suitable for unprinted overwrapping, offering unique as.. |
|||
Seal Strength | 200 - 410 g/25 mm | 200 - 410 g/in | Average value: 231 g/25 mm Grade Count:10 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Seal Strength | 200 - 810 g/25 mm @Temperature 80.0 - 140 °C |
200 - 810 g/in @Temperature 176 - 284 °F |
Average value: 419 g/25 mm Grade Count:65 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Seal Strength | 200 - 810 g/25 mm @Pressure 0.00345 - 0.276 MPa |
200 - 810 g/in @Pressure 0.500 - 40.0 psi |
Average value: 419 g/25 mm Grade Count:65 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |