Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 1% Secant Modulus, TD = 245 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 245 MPa
35500 psi
ASTM D882
ExxonMobil LD 051.LJ Shrink Film Resin  (discontinued **)
LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr..
1% Secant Modulus, TD 245 MPa
35500 psi
ASTM D882
ExxonMobil LD 051.LT Shrink Film Resin  (discontinued **)
LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr..
1% Secant Modulus, TD 245 MPa
35500 psi
ISO 178
Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film
LL 1810 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 H can be processed at high o..
1% Secant Modulus, TD 245 MPa
35500 psi
ISO 178
Total LLDPE LL 1810 Linear Low Density Polyethylene - Blown Film
LL 1810 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 can be processed at high outpu..
1% Secant Modulus, TD 245 MPa
35500 psi
ISO 178
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film
LL 1820 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 H can be processed at high o..
1% Secant Modulus, TD 245 MPa
35500 psi
ISO 178
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film
LL 1820 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 can be processed at high outpu..
1% Secant Modulus, TD 245 MPa
35500 psi
ASTM D882
Total Lotrene® Q1018N Linear Low Density Polyethylene, Blown Film
Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure..
1% Secant Modulus, TD 245 MPa
35500 psi
ASTM D882
Total Lotrene® Q2018C Linear Low Density Polyethylene, Blown Film
Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form ..
1% Secant Modulus, TD 245 MPa
35500 psi
ASTM D882
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film
Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form ..
1% Secant Modulus, TD 245 MPa
35500 psi
ASTM D882
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film
Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure..
1% Secant Modulus, TD 245 MPa
35500 psi
ASTM D882
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film
Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form ..
Copyright © lookpolymers.com All Rights Reserved