Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 215 MPa | 31200 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0225-B LDPE Clarity Film Resin
(discontinued **) Features: High optical clarityExcellent processability Applications: Produce and bakery filmLinersTextile packaging filmGeneral packaging requiring high clarity filmInformation provided by Nova Chem.. |
|||
1% Secant Modulus, MD | 215 MPa | 31200 psi | ISO 178 |
Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film LL 1810 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 H can be processed at high o.. |
|||
1% Secant Modulus, MD | 215 MPa | 31200 psi | ISO 178 |
Total LLDPE LL 1810 Linear Low Density Polyethylene - Blown Film LL 1810 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 can be processed at high outpu.. |
|||
1% Secant Modulus, MD | 215 MPa | 31200 psi | ISO 178 |
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film LL 1820 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 H can be processed at high o.. |
|||
1% Secant Modulus, MD | 215 MPa | 31200 psi | ISO 178 |
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film LL 1820 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 can be processed at high outpu.. |
|||
1% Secant Modulus, MD | 215 MPa | 31200 psi | ASTM D882 |
Total Lotrene® Q1018N Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
1% Secant Modulus, MD | 215 MPa | 31200 psi | ASTM D882 |
Total Lotrene® Q2018C Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
1% Secant Modulus, MD | 215 MPa | 31200 psi | ASTM D882 |
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
1% Secant Modulus, MD | 215 MPa | 31200 psi | ASTM D882 |
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
1% Secant Modulus, MD | 215 MPa | 31200 psi | ASTM D882 |
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |