Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 200 MPa | 29000 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 208 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LFH.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LFH 238 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 238 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion. It contains slip and antiblocking a.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
SABIC 218B Linear Low Density Polyethylene for Cast Film Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ISO 527-3 |
Polimeri Europa Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene Flexirene FF 25 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FF 25 is characterized by a high elongational viscosi.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | Blown Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE
(discontinued **) Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | Blown Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE
(discontinued **) Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer with enhanced stabilization packageCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use stra.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil LD 136.MV Packaging Film Resin
(discontinued **) LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0118-DP Butene Copolymer LLDPE Film Resin PF-0118-DP complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatu.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
LyondellBasell Petrothene® NA960000 Low Density Polyethylene ApplicationsPETROTHENE NA960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA960 exhibits good unif.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
LyondellBasell Petrothene® NA960070 Low Density Polyethylene ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
LyondellBasell Petrothene® NA960083 Low Density Polyethylene ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Westlake Hifor Xtreme SC74838 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74838 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and medium antiblock. Films produced with this re.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Westlake Hifor Xtreme SC74842 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74842 polymer is a high strength and good clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. Films produced wit.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7120B LLDPE Blown & Cast Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7120X Hexene Linear Low Density Polyethylene, Blown and Cast Film This LLDPE is tailored for cast film applications that require:Good stiffness at thin gaugesGood drawdownExcellent processabilityCan be used singly or in blends with LDPE or HDPEAvailable with slip .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | Cast Film at 1.25 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7120X Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for applications that require: Good stiffness at thin gaugesGood drawdownExcellent processabilityCan use straight or in blends with L.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil LD 103.59 Industrial Film Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil LDPE LD 103.59 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1236.85 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1236.86 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3001.63 Linear Low Density Polyethylene Resin Product Description: LL 3001.36 is a hexane copolymer LLDPE film resin. Films made from this resin have outstanding tensile and toughness properties. Superior strength properties, along with excell.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymer, medium slip, cast/blown film resinCharacteristics: good optics, good drawdown, can be used straight or blended with LDPE or HDPE, can b.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil Enable™ 20-10CH Metallocene Polyethylene Resin (Africa & Middle East Grade) Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Braskem Green PE SLH118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLH118 is a Linear Low Density Polyethylene, copolymer of hexene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Braskem LF0720/21AF Blown Film Extrusion Linear Low Density Polyethylene Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol® process technology. It shows low haze and high clarity associated with good balance of mechanical properties, processing .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM-D882 |
Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer LF118 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It is developed for blown film extrusion in blends with polyethylene. Films obtained with this p.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Braskem LH 118 LLDPE Blown Film Extrusion Polyethylene Description: LH118 is a Linear Low Density Polyethylene, copolymer of hexene-1, produced by Spherilene process. Developed for blown film extrusion in blends with polyethylenes. Films obtained with t.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Braskem LH118 Blown Film Extrusion Linear Low Density Polyethylene Stretch films; Liners; LDPE and HDPE blends; Packages for general use.Information provided by Braskem. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Braskem LL218/21 Cast Film Extrusion Linear Low Density Polyethylene Liners, LDPE and HDPE blends; General use packages; Technical films for automatic packaging.Additives: Antiblock, DInformation provided by Braskem. |