Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y320-C Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y320-D Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
LyondellBasell Petrothene® NA143063 Low Density Polyethylene ApplicationsPETROTHENE NA 143 is a series of homopolymer resins for blown film. Applications include stiff liners. Regulatory StatusNA 143 meets the requirements of the Food and Drug Administration.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
Westlake LF1040 Butene Linear Low Density Polyethylene Westlake LF1040 is a butene LLDPE resin with excellent mechanical and sealing properties. It can be used in stretch film and can liner applications, and is suitable for blending with LDPE in packagi.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil Enable™ 20-05CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-05CH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LL 1001x26 Blown Film Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LL 1001x72 Blown Film Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LL 1001x74 Blown Film Resin LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LL 1001x76 Blown Film Resin LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X31 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil NTX™ NTX 095 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil NTX™ NTX 104 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil NTX™ NTX 141 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil NTX™ NTX 150 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
1% Secant Modulus, MD | 193 MPa @Thickness 0.0250 mm |
28000 psi @Thickness 0.000984 in |
ASTM D882 |
Equate EFDA-7047 LLDPE Film Extrusion Resin EFDA-7047 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from this resin have good toughness, high tensile strength and puncture resistance. EFDA-7047 does n.. |
|||
1% Secant Modulus, MD | 193 MPa @Thickness 0.0250 mm |
28000 psi @Thickness 0.000984 in |
ASTM D882 |
Equate EFDC-7087 LLDPE Film Extrusion Resin EFDC-7087 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from EFDC-7087 have good toughness, high tensile strength and outstanding puncture resistance. EFDC-.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D-882 |
Bapolene® 200B Polyethylene, Film Extrusion Bapolene 200B is a low density polyethylene for blown film applications requiring superior clarity. It complies with US FDA 21CFR177.1520.Applications: General purpose, bakery, flexible, medical an.. |
|||
1% Secant Modulus, MD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LL 1001x59 Blown Film Resin
(discontinued **) LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical |