Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylac® EX28 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 62.1 - 86.0 MPa | 9000 - 12500 psi | Average value: 74.3 MPa Grade Count:10 |
Overview of materials for PVC, Sheet Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Flexural Yield Strength | 62.1 - 137 MPa | 9000 - 19800 psi | Average value: 111 MPa Grade Count:12 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Yield Strength | 62.1 - 82.7 MPa | 9000 - 12000 psi | ASTM D790 |
Premix Premi-Glas® 1201-10 Polyester SMC
(discontinued **) Premi-Glas® 1201-10 is a 10% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS.. |
|||
Flexural Yield Strength | 62.1 - 200 MPa | 9000 - 29000 psi | Average value: 79.9 MPa Grade Count:14 |
Overview of materials for Nylon 612 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app.. |
|||
Flexural Yield Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Spartech Royalite R722 PVC Alloy Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Spartech Royalite R86 PVC Acrylic Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Spartech SP-9050 Low Gloss ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Techmer ES HiFill® TPU GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Techmer ES Luriblend® PA4/6 HS TL15 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedUL File Number: E157318Information provided by TP Composites, Inc... |
|||
Flexural Yield Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Techmer ES Statiblend® ABS AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 62.1 MPa | 9000 psi | ASTM D790 |
PlastxWorld CEVIAN® E11 Inherently Static Dissipative ABS These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Clariant ABS4500 ABS, High Impact Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Clariant Renol PA2SP0010HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 62.1 - 89.6 MPa | 9000 - 13000 psi | Average value: 77.9 MPa Grade Count:23 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Yield Strength | 62.1 - 91.7 MPa | 9000 - 13300 psi | Average value: 78.0 MPa Grade Count:26 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Yield Strength | 62.1 - 370 MPa | 9000 - 53700 psi | Average value: 188 MPa Grade Count:43 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |