Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 57.0 MPa | 8270 psi | ASTM D790 |
Plaskolite Duraplex® 100% I Impact Modified Acrylic Sheet Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Flexural Yield Strength | 57.0 MPa | 8270 psi | ASTM D790 |
Plaskolite Duraplex® SG-10 Sign Grade Acrylic Sheet, Impact Modified Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Flexural Yield Strength | 57.0 MPa | 8270 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® EX39F ABS Highest impact extrusion ABS for sheet and blow molding applications. FDA food contact compliant. |
|||
Flexural Yield Strength | 57.0 MPa | 8270 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY CR3020 ASA Low-gloss ASA for profile and capstock applications |
|||
Flexural Yield Strength | 57.0 - 224 MPa | 8270 - 32500 psi | Average value: 132 MPa Grade Count:90 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Flexural Yield Strength | 57.0 MPa | 8270 psi | ISO 178 |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Flexural Yield Strength | 57.0 MPa | 8270 psi | at 5% strain; ASTM D790 |
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be.. |
|||
Flexural Yield Strength | 57.0 MPa | 8270 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
Flexural Yield Strength | 57.0 MPa | 8270 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+PS LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
Flexural Yield Strength | 57.0 - 160 MPa @Temperature -40.0 - 80.0 °C |
8270 - 23200 psi @Temperature -40.0 - 176 °F |
Average value: 113 MPa Grade Count:1 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Flexural Yield Strength | 57.0 MPa | 8270 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® EX39 ABS Highest impact extrusion ABS for sheet and blow molding applications. |
|||
Flexural Yield Strength | 57.0 - 97.0 MPa | 8270 - 14100 psi | Average value: 79.0 MPa Grade Count:6 |
Overview of materials for Acrylic, Impact Modified Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Yield Strength | 57.0 - 117 MPa | 8270 - 17000 psi | Average value: 97.6 MPa Grade Count:13 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |