Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 182.7 MPa | 26500 psi | ASTM D790 |
Plenco 51240 PET, Pellet, Injection Molded, Green
(discontinued **) PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P.. |
|||
Flexural Yield Strength | 183 MPa | 26500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V4860HR PBT 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Flexural Yield Strength | 183 MPa | 26500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare. |
|||
Flexural Yield Strength | 183 MPa | 26500 psi | ASTM D790 |
Techmer ES Plastiblend® PC/PBT GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 183 MPa | 26500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V4860HR PBT (Asia Pacific) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Flexural Yield Strength | 183 MPa | 26500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Flexural Yield Strength | 183 MPa | 26500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT LNP* THERMOCOMP* WF004 is a compound based on PBT resin containing 20% Glass Fiber. |
|||
Flexural Yield Strength | 183 MPa | 26500 psi | ASTM D790 |
Toyobo T-750 Nylon, Painting Grade Key Feature: Glass fiber and mineral reinforced, high heat distortion gradesInformation provided by Toyobo Co., Ltd |
|||
Flexural Yield Strength | 183 MPa | 26500 psi | ASTM D790 |
Chem Polymer Chemlon 125-15 MG Nylon 66, 25% Mineral/15% Glass Fiber Reinforced A 25% mineral reinforced, 15% glass fiber reinforced nylon 66 offering excellent rigidity, dimensional stability and tensile strength with improved warpage control in large area parts.Data provided .. |
|||
Flexural Yield Strength | 183 MPa | 26500 psi | ASTM D790 |
Chem Polymer Chemlon 130 GVH Nylon 66, 30% Glass Fiber Reinforced A glass fiber reinforced, flame retardant nylon 6,6 exhibiting excellent tensile strength and high temperature performance. The material has VO flammability rating according to UL94 testing procedu.. |
|||
Flexural Yield Strength | 183 MPa | 26500 psi | ASTM D790 |
Chem Polymer Durlex 730 G PBT, 30% Glass Fiber Reinforced A lubricated 30% glass reinforced PBT offering a balance of dimensional stability, tensile strength and high temperature performance.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 183 MPa | 26500 psi | |
Phenolic 40%, Carbon fabric 60% Phenolic - Monsanto "SC 1008". Carbon fabric - "CCA-1" |