Polymer Property : Flexural Yield Strength = 94.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS
Color package may affect performance. PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance.
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® BPL1000 PC
Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U..
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® BPL1000 PC (Europe-Africa-Middle East)
Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer
Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Asia Pacific)
Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Asia Pacific)
Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer
Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Asia Pacific)
Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer
Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® FXE1162T PC Copolymer (Europe-Africa-Middle East)
Lexan* FXE1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer
Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Europe-Africa-Middle East)
Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib..
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East)
Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope..
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® OQ3820 PC
High Viscosity, UV-stabilized grade for ophthalmic lenses.
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® OQ3820 PC (Asia Pacific)
High Viscosity, UV-stabilized grade for ophthalmic lenses.
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® SLX2571T PC Copolymer (Europe-Africa-Middle East)
Transparent weatherable PC copolymer for blowmolding/extrusion.
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Asia Pacific)
CY5100 is a Flame retardant PC blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® FXD104R PC (Asia Pacific)
FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties.
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific)
Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di..
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer
Transparent weatherable PC copolymer for blowmolding/extrusion.
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RZL36 PA 66 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RZL36 is a compound based on PA 66 resin containing Milled Glass, PTFE. Added features include: Internally Lubricated.
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Flexural Yield Strength 94.0 MPa
13600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer
Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with ..
Copyright © lookpolymers.com All Rights Reserved