Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 89.6 MPa @Thickness 3.17 mm |
13000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 89.6 MPa @Thickness 3.17 mm |
13000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 89.6 - 359 MPa | 13000 - 52000 psi | Average value: 152 MPa Grade Count:20 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Flexural Yield Strength | 89.6 - 138 MPa | 13000 - 20000 psi | Average value: 109 MPa Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Flexural Yield Strength | 89.6 MPa @Thickness 3.17 mm |
13000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 89.6 MPa @Thickness 3.17 mm |
13000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-(V) 10 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 89.6 - 372 MPa | 13000 - 54000 psi | Average value: 249 MPa Grade Count:13 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Techmer ES HiFill FR® PC FR SFX-ORANGE 1.0 Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantAppearance: OrangeInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Star Plastics PC731 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Star Plastics PC743 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Star Plastics PC7523R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Techmer ES HiFill® TPX-PBT-01022 25% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 25% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedInformation provided by TP Composites, .. |
|||
Flexural Yield Strength | 89.6 MPa @Thickness 3.17 mm |
13000 psi @Thickness 0.125 in |
|
Samyang Trirex® PC-3022U 15 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 89.6 MPa @Thickness 3.17 mm |
13000 psi @Thickness 0.125 in |
|
Samyang Trirex® PC-3025U 12 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Techmer ES HiFill FR® PC FR RD064 Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: RedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Techmer ES HiFill FR® PC FR SFX-GREEN 1.0 Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantAppearance: GreenInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Techmer ES HiFill® ABS HI 350 High Impact Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Density and High Impact ResistanceProcessing Method: Injection MoldingInformation provided by .. |
|||
Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Westlake Plastics Pomalux® Acetal Copolymer For Medical Applications Medical grade Pomalux is made from acetal copolymer resin which allows machined products the ability to retain dimensional integrity, maintain stability in water and most chemicals at elevated tempe.. |
|||
Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Clariant Renol BR7140 Polycarbonate/ABS Alloy Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
PlastxWorld Veroplas PA2001F Nylon 6 flame retarded (UL94 VO), unfilled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Techmer ES Electrafil® DB-50/SS/6 Polycarbonate, 6% Stainless Steel Fiber (dry blend) |