Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 78.0 MPa | 11300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® G360 ABS (Europe-Africa-Middle East) CYCOLAC G360 is a high flow, high impact, medium to high heat resistant injection moulding ABS grade. It is recommended for large or complex parts in the automotive or electrical power tool segments.. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Asia Pacific) High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Europe-Africa-Middle East) High impact PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC (Asia Pacific) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy XTWE280 ASA Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34E PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL346 is a compound based on Polycarbonate resin containing Glass Bead, PTFE. Added features of this material include: Easy Molding. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy XTWE280 ASA (Asia Pacific) Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 2 mm/min; ASTM D790 |
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound
(discontinued **) Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Asia Pacific) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Europe-Africa-Middle East) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 357 PBT+PC PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 3706 PBT+PC Impact modified PBT+PC resin. Outdoor enclosure. Not available in all colors. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® XD549S PBT+PC (Europe-Africa-Middle East) Xenoy XD549S is an automotive grade, designed for thin wall (2.5 mm.) direct gated exterior parts. The material has an excellent flow. Xenoy XD549S can be painted with primerless solvent or waterbas.. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | ASTM D790 |
Tipco Tipcolite® TEL 211 Phenolic Compound, Glass & Nylon Fibers, Soft Flow & Low Shrinkage Soft Flow Phenolic Compound, Reinforced with Glass & Nylon FibresApplications: Automotives & ElectricalProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industries L.. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | ASTM D790 |
Eastman Eastar MN058 Copolyester Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN058 Copolyester is a medical gra.. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | ASTM D790 |
Eastman Eastar MN059 Copolyester Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN059 Copolyester is a medical gra.. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 2 mm/min; ISO 178 |
Eurostar Staramide PX08000 PA6, Impact Modified, Injection Molded Staramide PX08000 is an Impact Modified Polyamide 6 Injection Molding Resin (also known as Star X 2006)Information provided by Eurostar. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 2 mm/min; ASTM D790 |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Flexural Yield Strength | 78.0 - 245 MPa | 11300 - 35500 psi | Average value: 124 MPa Grade Count:18 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermotuf PX08000 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* PX08000 is a compound based on PA6 resin containing Impact Modifier. Added features include : High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region... |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON ME006 PP LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Yield Strength | 78.0 MPa | 11300 psi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl EN212 PPE+PS Extrusion grade. 212F (100C) DTUL. UL94 V-1 rated.This data was supplied by SABIC-IP for the Americas region. |