Mechanical Properties Metric English Comments
Flexural Yield Strength 64.7 MPa

@Thickness 3.20 mm
9390 psi

@Thickness 0.126 in
15mm/min; ASTM D790
LG Chemical LI933 Co-Extrusion ASA
Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical
Flexural Yield Strength 64.7 MPa

@Thickness 3.20 mm
9390 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance
Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG ..
Flexural Yield Strength 64.7 MPa

@Thickness 3.20 mm
9390 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUCEL HI510 POM+Rubber, High Impact
Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0Information provided by LG Chemical
Flexural Yield Strength 64.7 MPa

@Thickness 3.20 mm
9390 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical PT270 ABS
Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 64.7 MPa

@Temperature 23.0 °C
9390 psi

@Temperature 73.4 °F
ASTM D790
IRPC Polimaxx Porene AN510 Acrylonitrile Butadiene Styrene
Applications:injection moldingelectrical appliances such as microwaves, computers, tv, switch boxes, switch panels, etc.automotive componenets
Flexural Yield Strength 64.7 MPa

@Temperature 23.0 °C
9390 psi

@Temperature 73.4 °F
ASTM D790
IRPC Polimaxx Porene KU200 Acrylonitrile Butadiene Styrene
Applications:extrusion applicationautomotive parts such as instrument panels, console boxes, switches, automotive louvers, ectelectrical appliances
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron AP-78 EP ABS Electro Plating Applications
Electroplating & Hot Stamping GradesInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron HR-105 ABS Super Heat Resistant
High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron HR-59(M) ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D790
Bhansali Engineering Abstron IM-11 ABS Injection Molding Grade
High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade
High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D790
Bhansali Engineering Abstron KU-600 ABS Super Heat Resistant
High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron AP-78 EP ABS Electro Plating Applications
Electroplating & Hot Stamping GradesInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron SE-20P ABS Sheet Extrusion Grade
ABS Pipe GradeInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade
Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron SE-20P ABS Sheet Extrusion Grade
ABS Pipe GradeInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D790
Bhansali Engineering Abstron IM-11 ABS Injection Molding Grade
High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D790
Bhansali Engineering Abstron KU-600 ABS Super Heat Resistant
High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron KU600N ABS Heat Resistant
High ImpactInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron HR-105 ABS Super Heat Resistant
High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron HR-59(M) ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade
High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron KU600N ABS Heat Resistant
High ImpactInformation provided by Bhansali
Flexural Yield Strength 64.7 MPa

@Thickness 6.40 mm
9390 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade
Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali
Copyright © lookpolymers.com All Rights Reserved