Mechanical Properties Metric English Comments
Flexural Yield Strength 57.0 MPa
8270 psi
ASTM D790
Plaskolite Duraplex® 100% I Impact Modified Acrylic Sheet
Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc.
Flexural Yield Strength 57.0 MPa
8270 psi
ASTM D790
Plaskolite Duraplex® SG-10 Sign Grade Acrylic Sheet, Impact Modified
Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc.
Flexural Yield Strength 57.0 MPa
8270 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycolac® EX39F ABS
Highest impact extrusion ABS for sheet and blow molding applications. FDA food contact compliant.
Flexural Yield Strength 57.0 MPa
8270 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics GELOY CR3020 ASA
Low-gloss ASA for profile and capstock applications
Flexural Yield Strength 57.0 - 224 MPa
8270 - 32500 psi
Average value: 132 MPa Grade Count:90
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Flexural Yield Strength 57.0 MPa
8270 psi
ISO 178
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade
Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®..
Flexural Yield Strength 57.0 MPa
8270 psi
at 5% strain; ASTM D790
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned
Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be..
Flexural Yield Strength 57.0 MPa
8270 psi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East)
LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics.
Flexural Yield Strength 57.0 MPa
8270 psi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+PS
LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics.
Flexural Yield Strength 57.0 - 160 MPa

@Temperature -40.0 - 80.0 °C
8270 - 23200 psi

@Temperature -40.0 - 176 °F
Average value: 113 MPa Grade Count:1
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
Flexural Yield Strength 57.0 MPa
8270 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycolac® EX39 ABS
Highest impact extrusion ABS for sheet and blow molding applications.
Flexural Yield Strength 57.0 - 97.0 MPa
8270 - 14100 psi
Average value: 79.0 MPa Grade Count:6
Overview of materials for Acrylic, Impact Modified Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of..
Flexural Yield Strength 57.0 - 117 MPa
8270 - 17000 psi
Average value: 97.6 MPa Grade Count:13
Overview of materials for Acrylic, Optical Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr..