Flexural Yield Strength 34.5 MPa
5000 psi
ASTM D790
Multibase Multi-Pro® 2510 XGW Polypropylene
Mineral Filled, 27% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Flexural Yield Strength 34.5 - 128 MPa
5000 - 18500 psi
Average value: 91.6 MPa Grade Count:20
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..
Flexural Yield Strength 34.5 - 75.8 MPa
5000 - 11000 psi
Average value: 59.6 MPa Grade Count:21
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max..
Flexural Yield Strength 34.5 MPa
5000 psi
ASTM D790
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Flexural Yield Strength 34.5 MPa
5000 psi
ASTM D790
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Flexural Yield Strength 34.5 MPa
5000 psi
ASTM D790
Techmer ES HiFill® PP 0159 Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Flexural Yield Strength 34.5 MPa
5000 psi
ASTM D790
Techmer ES HiFill® PP GB10 10% Glass Beads Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightInformation provided by TP Composites, Inc.
Flexural Yield Strength 34.5 MPa
5000 psi
ASTM D790
PlastxWorld DAICEL STYROL® GH10 HIPS
High heat resistance and flame retarded HIPS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Yield Strength 34.5 MPa
5000 psi
ASTM D790
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Copyright © lookpolymers.com All Rights Reserved