Mechanical Properties Metric English Comments
Flexural Yield Strength 216 MPa
31300 psi
DIN 53455; ASTM D790
Kolon SPESIN® KP213G45 Flame Retardant PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..
Flexural Yield Strength 216 MPa
31300 psi
DIN 53455; ASTM D790
Kolon SPESIN® KP2122G30VO G/F Reinforced & Retardant PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..
Flexural Yield Strength 216 - 425 MPa
31300 - 61600 psi
Average value: 326 MPa Grade Count:106
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Flexural Yield Strength 216 MPa

@Thickness 6.40 mm
31300 psi

@Thickness 0.252 in
3mm/min; ASTM D790
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose
Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General PurposeApplication: HMID, SLMP B, HolderCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Flexural Yield Strength 216 MPa

@Thickness 3.20 mm
31300 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant
Feature: Injection Molding, PA66+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
Flexural Yield Strength 216 MPa
31300 psi
DIN 53455; ASTM D790
Kolon SPESIN® KP513G30WBL Multi Reinforced PBT Resin
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High..
Flexural Yield Strength 216 MPa
31300 psi
DIN 53455; ASTM D790
Kolon KOPA® KN133G20 G/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Yield Strength 216 MPa
31300 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® T101G36 PET, 36% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Flexural Yield Strength 216 MPa
31300 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Flexural Yield Strength 216 MPa
31300 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® T101G36 PET, 36% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Flexural Yield Strength 216 MPa
31300 psi
ASTM D790
Toyobo Vylopet® EMC330K Glass Reinforced Polyester, Easy Molding Grade
HB UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, c..
Flexural Yield Strength 216 MPa
31300 psi
ASTM D790
Cheng Yu Plastic N6GV15 Flame Retardant Nylon 6, 15% Glass Filled
Flexural Yield Strength 216 MPa
31300 psi
ASTM D790
Cheng Yu Plastic FR200GV45 Flame Retardant Nylon 66, 45% Glass Fiber
Flexural Yield Strength 216 MPa
31300 psi
ASTM D790
A. Schulman ComAlloy E-16674B PPS, Electrically Conductive - Carbon Fiber Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Yield Strength 216 MPa
31300 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Verton PV007SV_YW8D151 PA 6
Preliminary data for 35% long fiber single pellet color filled PA6This data was supplied by SABIC-IP for the Americas region.
Flexural Yield Strength 216 MPa
31300 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Copyright © lookpolymers.com All Rights Reserved