Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 34.5 MPa | 5000 psi | ASTM D882 |
Formosa Plastics Formolene® FORMAX® L91507A Film (Hexene Grade) LLDPE
(discontinued **) Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. .. |
|||
Film Tensile Strength at Break, TD | 34.5 MPa | 5000 psi | ASTM D882 |
Formosa Plastics Formolene® FORMAX® L91507E2 Film (Hexene Grade) LLDPE
(discontinued **) Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. .. |
|||
Film Tensile Strength at Break, TD | 34.5 MPa | 5000 psi | ASTM D882 |
Formosa Plastics Formolene® FORMAX® L91507H Film (Hexene Grade) LLDPE
(discontinued **) Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. .. |
|||
Film Tensile Strength at Break, TD | 34.5 MPa | 5000 psi | ASTM D882 |
M. Holland Company MAGMA® LL1091 LLDPE
(discontinued **) Features: Good Heat Seal, Good ToughnessUses: PackagingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Film Tensile Strength at Break, TD | 34.5 - 41.4 MPa | 5000 - 6000 psi | ASTM D882 |
Honeywell ACLAR® 11A (8.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, TD | 34.5 - 41.4 MPa | 5000 - 6000 psi | ASTM D882 |
Honeywell ACLAR® 11A (4.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, TD | 34.5 - 55.2 MPa | 5000 - 8000 psi | ASTM D882 |
Honeywell ACLAR® 22A (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provide.. |
|||
Film Tensile Strength at Break, TD | 34.5 - 55.2 MPa | 5000 - 8000 psi | ASTM D882 |
Honeywell ACLAR® 22A (1.50 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provide.. |
|||
Film Tensile Strength at Break, TD | 34.5 - 48.3 MPa | 5000 - 7000 psi | ASTM D882 |
Honeywell ACLAR® 22C (3.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Film Tensile Strength at Break, TD | 34.5 - 48.3 MPa | 5000 - 7000 psi | ASTM D882 |
Honeywell ACLAR® 22C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Film Tensile Strength at Break, TD | 34.5 MPa | 5000 psi | ASTM D882 |
LyondellBasell Alathon® L5005 High Density Polyethylene ApplicationsALATHON L 5005 is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typi.. |
|||
Film Tensile Strength at Break, TD | 34.5 MPa @Thickness 0.0254 mm |
5000 psi @Thickness 0.00100 in |
ASTM D882A |
Total L425 HDPE Film Blown film polyethylene grade. Provides excellent bubble stability, exceptional tear strength, high impact and puncture resistance, outstanding clarity and gloss, good stiffness, excellent compatibi.. |
|||
Film Tensile Strength at Break, TD | 34.47 MPa | 5000 psi | ASTM D882 |
Formosa Plastics Formolene® L62022B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cast stretch film and high quality packaging films requiring clarity and toughness.A Hexene Copolymer Linear Low Density Polyethylene for film applications i.. |
|||
Film Tensile Strength at Break, TD | 34.5 MPa | 5000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3404.48 Linear Low Density Polyethylene Resin Product Description: LL 3404.48 is a hexane medium density polyethylene cast film grade for applications requiring high strength and high stiffness. Films produced from this resin exhibit good tensi.. |
|||
Film Tensile Strength at Break, TD | 34.5 MPa | 5000 psi | |
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2036A Polyethylene resin is a cast film polymer having improved thermal stability for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a for food .. |
|||
Film Tensile Strength at Break, TD | 34.5 MPa | 5000 psi | ASTM D882 |
ExxonMobil Escorene™ 768.MJ Blown Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 768.MJ is a low gel 26.2% vinyl acetate copolymer designed for film and compounding applications. This resin provides very low modulus films with high tensile .. |
|||
Film Tensile Strength at Break, TD | >= 34.5 MPa | >= 5000 psi | ASTM D 882 A |
Total Finathene® HL 328 HDPE resin
(discontinued **) Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusionInformation provided provided by .. |
|||
Film Tensile Strength at Break, TD | 34.5 MPa | 5000 psi | ASTM D882 |
M. Holland Company MAGMA® LM115-C LLDPE