Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 200 - 283 MPa | 29000 - 41000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film
(discontinued **) Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many .. |
|||
Film Tensile Strength at Break, TD | 200 - 283 MPa | 29000 - 41000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 1500 Clear Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr.. |
|||
Film Tensile Strength at Break, TD | 200 - 283 MPa | 29000 - 41000 psi | ASTM D882 |
Honeywell Capran® Emblem™ MT1500 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ MT1500 is a 0.60 mil (15 micron) biaxially oriented nylon 6 film with a metallized barrier coating well suited for high barrier packaging applications. Informati.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882 |
Honeywell Oxyshieldâ„¢ BOEB Biaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshieldâ„¢ BOEB is a 0.60 mil (15 micron) biaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relative humidity. T.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 440LL-201 OPP Film Product Description: A matte finish, clear, one-side treated, polypropylene film intended for use as an overlaminate in pressure-sensitive labeling applications. It presents an appealing paper-like,.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Oppalyte™ 35MD447 OPP Film Product Description: A coextruded super white opaque, modified high density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for use.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 515 Polyester Film A high clarity film which is two side pretreated for slip to combine good handling properties with high clarity and brilliance.Typical Applications: MELINEX® 515 is suitable for applications which .. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Melinex® ST579 Polyester Film, 200 Gauge Melinex® ST579 is a clear, heat stabilized polyester film that is primed on one surface for adhesion. Typical applications include flexible electronics, touch screens, displays, circuitry, and othe.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 850H Polyester Film, 48 Gauge Mylar® 850H (also called Mylar® 850) is a co-extruded, one side amorphous, heat sealable polyester film designed to be used in metallized, print, and lamination applications. This film is suitable.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 854 Polyester Packaging Film, 60 Gauge Data provided by DuPont Packaging Polymers.DuPont Melinex® DuPont Melinex® 854 is a clear, one side coextruded heat sealable surface similar to Melinex® 850. The opposite surface is adhesion pret.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL21 Polyester Film, 1000 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MDA Polyester Film, 1000 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MO21 Polyester Film, 1000 Gauge Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MO21 Polyester Film, 900 Gauge Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® OL22 Polyester Film, 100 Gauge Product Description: Mylar® OL22 is a one side heat sealable, polyester film. It can be heat sealed to itself and heat seals well to thermoformed APET/CPET trays and APET coated board. It also heat.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® OWF Polyester Film, 48 Gauge Product Description: Mylar® OWF is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. This film is suitable for use in contact with food. Appro.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® OWF Polyester Film, 80 Gauge Product Description: Mylar® OWF is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. This film is suitable for use in contact with food. Appro.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 440LLG201 OPP Film Product Description: A matte, clear, one-side treated, polypropylene film intended to be used as the outer web of a lamination in roll-fed labeling applications. It presents an appealing paper-like,.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Melinex® ST580 Polyester Film, 200 Gauge Melinex® ST580 is a clear, heat stabilized polyester film that is primed on one surface for enhanced adhesion to UV curable inks and coatings. Typical applications include flexible electronics, tou.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 850H Polyester Film, 80 Gauge Mylar® 850H (also called Mylar® 850) is a co-extruded, one side amorphous, heat sealable polyester film designed to be used in metallized, print, and lamination applications. This film is suitable.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® A Polyester Film, 900 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL21 Polyester Film, 900 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MDA Polyester Film, 900 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Oppalyte™ 30MD447 OPP Film Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u.. |
|||
Film Tensile Strength at Break, TD | 200 MPa | 29000 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Oppalyte™ 40MD447 OPP Film Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u.. |