Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 130 g | 0.287 lb | F-50 at 26 in.; ASTM D1709 |
Chevron Phillips 7109BK Linear low density polyethylene blown film resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer, blow film resin, medium slip, medium antiblock version of 7109Characteristics: good stiffness at thin gauges, good drawdown, low COF, c.. |
|||
Dart Drop Test | 130 g | 0.287 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
Iran Petrochemical (PCC) Arak 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
Iran Petrochemical (PCC) Tabriz 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Dart Drop Test | >= 130 g | >= 0.287 lb | ASTM D1709 |
Iran Petrochemical (PCC) Bandar Imam Poliran LH0050 LDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D 1709 A |
Total Finathene® DF 210 HDPE resin
(discontinued **) Applications: Irrigation tape and tubingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |
|||
Dart Drop Test | 130 g | 0.287 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar.. |
|||
Dart Drop Test | 130 g | 0.287 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA963083 Low Density Polyethylene ApplicationsPETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellen.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
Iran Petrochemical (PCC) LL0220AA Linear Low Density Polyethylene LL 0220 AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. This grade is suitable for the production of blown film for light duty applications and for the production of ca.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ L1810F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesContains 1600 ppm slip agent and 1900 ppm antiblocking agentRecommended Applications:Film for heavy duty bag, industrial bag, rice bag, su.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ L2009F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ L2009FA Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains no slip agent and antiblocking agentRecommended App.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ LD1905F Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE, LLDPEContains 1500 ppm slip agent and 2600 ppm antiblocking agentRecommended Applications:General purpose bagVeg.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ LD1905FA Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ISO 7765-1 |
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film LL 1820 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 H can be processed at high o.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ISO 7765-1 |
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film LL 1820 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 can be processed at high outpu.. |
|||
Dart Drop Test | >= 130 g | >= 0.287 lb | 20µm film, HDPE |
Total HT 514 MDPE film Finathene® HT 514 is a medium density polyethylene produced by the slurry loop low pressure polymerization process. Finathene® HT 514 can be used alone, blended or coextruded in a wide variety of .. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
ExxonMobil Enable™ 27-03CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709A |
ExxonMobil Enable™ 27-05HH Metallocene Polyethylene Resin Product Description: Enable 27-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709A |
ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin Product Description: Nexxstar 00328 is an LDPE grade, which offers good film rigidity combined with very good optical properties. Its primary use is for high performance collation shrunk packaging.A.. |
|||
Dart Drop Test | 130 g | 0.287 lb | Method A; ASTM D1709 |
Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-1003 NT 7 is an ethylene-hexene-1 copolymer, design.. |
|||
Dart Drop Test | 130 g | 0.287 lb | g/F50; ASTM D1709 |
Braskem Green PE SLL118/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL118/21 is a LLDPE Butene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties .. |
|||
Dart Drop Test | 130 g | 0.287 lb | gF/50%f; ASTM D1709 |
Braskem LF0720/21AF Blown Film Extrusion Linear Low Density Polyethylene Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol® process technology. It shows low haze and high clarity associated with good balance of mechanical properties, processing .. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM-D1709 |
Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer LL4800N is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process. It was developed for cast film extrusion. Films obtained with this product show a good processi.. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM-D1709 |
Braskem LL6802N LLDPE Blown Film Extrusion Polyethylene Copolymer LL6802N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing aid .. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D 1709 A |
Total Finathene® HL 328 HDPE resin
(discontinued **) Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusionInformation provided provided by .. |
|||
Dart Drop Test | 130 g | 0.287 lb | ASTM D1709 |
Huntsman PE 1253 EVA Film Extrusion
(discontinued **) 2.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, good heat seal characteristics.Applications: Film extrusion: general purpose packaging where to.. |
|||
Dart Drop Test | 130 g | 0.287 lb | 50µ; ISO 7765-1 |
Total Lacqtene® 1025 FH 24 LDPE blown film
(discontinued **) Radical polyethylene made by high pressure tubular process. Slip and antiblock formulated grade for good transparent thin films. Advised temperature profile : 150 to 190°C.Information provided prov.. |
|||
Dart Drop Test | 130 g @Thickness 0.0400 mm |
0.287 lb @Thickness 0.00157 in |
ISO 7765-1 |
Borealis Borstar® FB4370 Medium Density Polyethylene Borstar® FB4370 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Applications: Borstar® FB4370 has been developed especially for ap.. |