Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | >= 95.0 g | >= 0.209 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | 95.0 g | 0.209 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin; 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have.. |
|||
Dart Drop Test | >= 95.0 g | >= 0.209 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | 95.0 g | 0.209 lb | ASTM D1709 |
Huntsman PE1155 EVA Film Extrusion
(discontinued **) 1.5% Vinyl Acetate EVA Copolymer and FDA compliant.Features: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications:.. |
|||
Dart Drop Test | 95.0 g | 0.209 lb | ISO 7765-1 |
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of.. |
|||
Dart Drop Test | 95.0 g @Thickness 0.0356 mm |
0.209 lb @Thickness 0.00140 in |
F<sub>50</sub>; ASTM D-1709 |
Bapolene® 270F Low Density Polyethylene Film Extrusion Resin Bapolene® 270F is an LDPE for blown film requiring superior clarity. It contains 1600 ppm antiblock and 725 ppm slip additives. This product meets the Food and Drug Administration requirements of .. |
|||
Dart Drop Test | 95.0 g | 0.209 lb | ISO 7765-1 |
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene.. |