Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 80.0 g | 0.176 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FM 50 Low Density Polyethylene - Blown Film Extrusion Riblene FM 50 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FM 50 is characterized by optimum optical properties and rigidity.Films manufactured with Riblene FM 50.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FM 53 Low Density Polyethylene - Blown Film Extrusion Riblene FM 53 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 53 is characterized by optimum optical properties and rigid.. |
|||
Dart Drop Test | >= 80.0 g | >= 0.176 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 4116Q (16403) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | >= 80.0 g | >= 0.176 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 4121N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | 80.0 g | 0.176 lb | |
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | |
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM D1709 |
M. Holland Company LL104 LLDPE
(discontinued **) Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM D1709 |
ExxonMobil LD 117.03 Blown Overwrap Film Resin
(discontinued **) LD 117 resins are homopolymer film resins with good clarity and excellent stiffness. Film from LD 117 resins can be used in overwrap applications and push-through type packaging equipment. Film ma.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM D1709 |
Huntsman PE1020 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Medium impact strength and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 .. |
|||
Dart Drop Test | >= 80.0 g | >= 0.176 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 4118P (18402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM D1709 |
Iran Petrochemical (PCC) LL22501 Linear Low Density Polyethylene 22501 is a high stiffness LLDPE blown film grade designed for applications requiring good optical properties even at low extrusion temperature. This resin combines ease of processing with low gels a.. |
|||
Dart Drop Test | <= 80.0 g | <= 0.176 lb | ASTM D1709 |
Solvay Specialty Polymers Ajediumâ„¢ Films -- Polyetherimide Polyether Imide (PEI) Films of polyetherimide (PEI) are amorphous and suitable for high temperature applications. They have an excellent combination of thermal, mechanical and electrical properties, along with very low f.. |
|||
Dart Drop Test | 80.0 g @Thickness 0.0400 mm |
0.176 lb @Thickness 0.00157 in |
ISO 7765-1 |
Borealis FA7220 Low Density Polyethylene FA7220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for production of blown film or cast film with good optical properties. When cast on a polish.. |
|||
Dart Drop Test | 80.0 g @Thickness 0.0400 mm |
0.176 lb @Thickness 0.00157 in |
ISO 7765-1 |
Borealis FA7224 Low Density Polyethylene FA7224 has been developed for applications such as: Thin bags with excellent optical and slip properties, and laundry and other textile bags. Contains antioxidant.Information provided by Borealis AG.. |
|||
Dart Drop Test | 80.0 g @Thickness 0.0400 mm |
0.176 lb @Thickness 0.00157 in |
ISO 7765-1 |
Borealis FA7229 Low Density Polyethylene FA7229 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant and Cling additive. Applications: food wrap film, lamination films, blending, and other blown cling film.Information pr.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ISO 7765-1 |
Total PPH 4026 Polypropylene Homopolymer, Film Polypropylene PPH 4026 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min for the cast extrusion of films with outstanding stiffness and heat resistance.Polypropylene PPH 4026 is in.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | 40µm film, LDPE |
Total HT 514 MDPE film Finathene® HT 514 is a medium density polyethylene produced by the slurry loop low pressure polymerization process. Finathene® HT 514 can be used alone, blended or coextruded in a wide variety of .. |
|||
Dart Drop Test | <= 80.0 g | <= 0.176 lb | ASTM D1709 |
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin Product Description: Enable 35-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Dart Drop Test | <= 80.0 g | <= 0.176 lb | ASTM D1709 |
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 35-05HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM D1709A |
ExxonMobil LDPE LD 100.BW Low Density Polyethylene Resin Product Description: LD 100.BW is a LDPE grade, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.Ava.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM D1709A |
ExxonMobil LDPE LD 100BR Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM D1709A |
ExxonMobil LDPE LD 117.85 Low Density Polyethylene Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM D1709A |
ExxonMobil LDPE LD 158BW Low Density Polyethylene Resin Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel .. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM D1709A |
ExxonMobil LDPE LD 158JD Low Density Polyethylene Resin Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel .. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM D1709A |
ExxonMobil LDPE LD 185BW Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM D1709A |
ExxonMobil LDPE LGA 105 Low Density Polyethylene Resin Product Description: LGA 105 is a homopolymer, garment film resin with good toughness. It is capable of being draw-down to thin gauges.Availability: North America Additive: Antiblock: NoSlip: NoPro.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM D1709A |
ExxonMobil LLDPE LL 3001.32 Cast Linear Low Density Polyethylene Resin Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM-D1709 |
Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer FG31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for blown film extrusion in blends with polyethylene. Films obtained with this pr.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM-D1709 |
Braskem LF218/21 LLDPE Cast and Blown Film Extrusion Polyethylene Copolymer LF218/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and optical prope.. |
|||
Dart Drop Test | 80.0 g | 0.176 lb | ASTM D1709 |
ExxonMobil Enable™ 35-05CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 35-05CH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |