Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 60.0 g | 0.132 lb | F50; ISO 7765-1 |
Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 are characterized by an.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | F50; ISO 7765-1 |
Polimeri Europa Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 U are characterized b.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709 |
SABIC HP4023W Low Density Polyethylene for Blown Film Product Description: HP4023W is a Low Density Polyethylene grade suitable for producing general purpose films and contains slip and antiblock additives. It yields excellent processability with goo.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-108 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer high clarity film resin with a good balance of toughness, stiffness, and drawdown capability. This resin has good machinability in ba.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | F; ASTM D1708/A |
M. Holland Company LD220 LDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good ToughnessUses: Industrial Applications, Liners, PackagingProcessing Method: Blown FilmInformation provided by M. Holland. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-117 MDPE Blown Overwrap Film Resin, Tough
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-117 can be used in overwrap applications and in push-through .. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-129 MDPE Cast Overwrap Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-129 can be used in overwrap applications and in push-through .. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA271009 Medium Density Polyethylene ApplicationsPETROTHENE NA 271-009 is a medium density polyethylene resin designed to overwrap film applications. NA 271-009 exhibits good film optics and high stiffness. Regulatory StatusNA 271-009.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA285003 Medium Density Polyethylene ApplicationsPETROTHENE NA 285-003 is a medium density polyethylene resin for blown or cast film extrusion. Typical applications include overwrap film. This product exhibits good film optics and hi.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709 |
LG Chemical SEETEC BF500 LDPE Characteristics: Good Processability and Good Optical Properties Additives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG Chem.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709 |
ExxonMobil LD 102.LC Thin Gauged Film Resin L Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawndown to thing gauges.Availability: Latin America, North America and .. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709A |
ExxonMobil LDPE LD 102.LC Low Density Polyethylene Resin Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawn down to thing gauges.Availability: Latin America, North America and S.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709A |
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709A |
ExxonMobil LDPE LD 151BW Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709A |
ExxonMobil LDPE LD 151GZ Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709A |
ExxonMobil LDPE LD 151HR Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709A |
ExxonMobil LDPE LD 152BW Low Density Polyethylene Resin Product Description: LD 152BW is an LDPE grade offering an excellent combination of optical properties and stiffness. The 2.2 MI makes it ideal for blowing thicker films.Availability: Africa & Middl.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1001.32 Linear Low Density Polyethylene Resin Product Description: LL 1001.32 is a butane LLDPE resin. Films made from LL 1001.32 have very good tensile and toughness properties.Availability: Latin America, North America and South America Addit.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1107X93 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1107X95 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM-D1709 |
Braskem F2523 LDPE Blown Film Extrusion Polyethylene LDPE F2523 is a low-density polyethylene. It has good sealing characteristics, optical, and mechanical properties. It contains antiblock and slip additives. Its applications include general purpose .. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM-D1709 |
Braskem LF320 LLDPE Cast Film Extrusion Polyethylene Copolymer LF320 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It was developed for cast film extrusion. Films obtained with this product show a good processin.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM-D1709 |
Braskem PB681 LDPE Cast and Blown Film Extrusion, Injection Molding Polyethylene PB681 is a resin produced under high pressure in a tubular reactor. This resin presents excellent 'draw down' (stability to form fine films). The films produced with this resin have excellent optica.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | gF/50%f; ASTM D1709 |
Braskem PB681/59 Blown Film Extrusion Low Density Polyethylene Description: PB681/59 is a grade produced under high pressure in a tubular reactor. This resin is used for laminating films mainly on paper substrate. It is also used in the extrusion coating proces.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | g/F50; ASTM D1709 |
Braskem BF2021 Cast Film Extrusion Low Density Polyethylene Films for diapers and absorbent articles; Medium resistance films or for general use.Information provided by Braskem. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | Method F; ASTM D1708/A |
M. Holland Company LD220MM LDPE
(discontinued **) Additives: Medium Antiblock, SlipFeatures: Medium Antiblocking, Good Heat Seal, Medium SlipUses: Liners, PackagingProcessing Method: Blown FilmInformation provided by M. Holland. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709, A |
Total Lumicene® mPE M 3410 EP Metallocene Medium Density Film Resin
(Unverified Data**) Polyethylene: Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityHigh StiffnessGood puncture resistanceGood tear strengthGood heat sealing p.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709 |
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made from Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. The.. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | gF/50%f; ASTM D1709 |
Braskem F2523 Blown Film Extrusion Low Density Polyethylene Automatic packaging for several products; High transparency films.Additives: Antiblock, DInformation provided by Braskem. |
|||
Dart Drop Test | 60.0 g | 0.132 lb | ASTM D1709 |
SABIC HP2022 Series Low Density Polyethylene for Blown Film Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:.. |