Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 50.0 g | 0.110 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® FH 50 Linear Medium Density Polyethylene Clearflex FH 50 is a linear medium density polyethylene, with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FH 50 are characterized by a good balance between toug.. |
|||
Dart Drop Test | 50.0 g | 0.110 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-138 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin offering good clarity, toughness, and stiffness. Blown film made from this resin has good machinability in bag equipment a.. |
|||
Dart Drop Test | 50.0 g | 0.110 lb | ASTM D1709 |
Huntsman PE1037 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Medium clarity packaging film and good draw down characteristics.Applications: Film extrusion: general purpose packaging and film applications.FDA Notes: Con.. |
|||
Dart Drop Test | 50.0 g | 0.110 lb | ASTM D1709 |
Huntsman PE1044 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA reg.. |
|||
Dart Drop Test | 50.0 g | 0.110 lb | ASTM D1709 |
Huntsman PE1065 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA regu.. |
|||
Dart Drop Test | 50.0 - 60.0 g | 0.110 - 0.132 lb | ASTM D1709 |
LyondellBasell Petrothene® M2520FN Low Density Polyethylene ApplicationsPETROTHENE M 2520 is a film grade resin that exhibits excellent optics, good gloss and good bubble stability. A typical application for this resin is high clarity packaging. Regulatory.. |
|||
Dart Drop Test | 50.0 g | 0.110 lb | ISO 7765-1 |
Borealis FL5580 High Density Polyethylene FL5580 is a high density polyethylene with an excellent combination of extrusion properties and moisture barrier properties. Applications: FL5580 has been developed especially for applications like.. |
|||
Dart Drop Test | <= 50.0 g | <= 0.110 lb | 1.0 mil; ASTM D1709A |
Total 9458 HDPE Film Grade Medium molecular weight grade. Excellent bubble stability, good compatibility with LDPE and LLDPE, good heat resistance, high stiffness and tensile strength.Applications: Release liners, Stand-up ba.. |
|||
Dart Drop Test | >= 50.0 g | >= 0.110 lb | ASTM D1709, A |
Total HDPE HL 535 High Density Polyethylene, Film Resin Polyethylene: Medium molecular weight, high density film resinCharacteristics:High stiffnessGood heat resistanceExcellent bubble stabilityGood compatibility with LDPE and LLDPEApplications:Release .. |
|||
Dart Drop Test | >= 50.0 g | >= 0.110 lb | 20µm; ASTM D 1709 |
Total Lumicene® M 3410 EP HDPE Film, sheet FINACENE® M 3410 EP is a medium density metallocene based polyethylene resin. FINACENE® M 3410 EP is especially dedicated to film applications where a higher rigidity, good transparency and shrink.. |
|||
Dart Drop Test | <= 50.0 g | <= 0.110 lb | ASTM D1709,A |
Total MDPE HL 323 Medium Density Polyethylene, Film Resin Medium molecular weight, medium density film resinCharacteristics:Excellent balance of stiffness and impact strengthGood puncture resistanceExcellent compatibility with LDPE and LLDPEGood tensile st.. |
|||
Dart Drop Test | <= 50.0 g | <= 0.110 lb | 1.0 mil; 2.5 BUR; ASTM D1709A |
Total HL 428 HDPE Film Grade Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro.. |
|||
Dart Drop Test | <= 50.0 g | <= 0.110 lb | ASTM D1709A |
ExxonMobil HDPE HD 7925.30 High Density Polyethylene Resin Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements.A.. |
|||
Dart Drop Test | <= 50.0 g | <= 0.110 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1002YB Cast Linear Low Density Polyethylene Resin Product Description: LL 1002YB is an LLDPE resin designed for cast films. It offers high gloss and excellent drawdown in both blown and cast film applications. LL 1002YB may also be used as a blend .. |
|||
Dart Drop Test | <= 50.0 g | <= 0.110 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1236.85 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
Dart Drop Test | <= 50.0 g | <= 0.110 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1236.86 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
Dart Drop Test | <= 50.0 g | <= 0.110 lb | ASTM D1709A |
ExxonMobil LLDPE LL 3402.48 Blown Linear Low Density Polyethylene Resin Product Description: LL 3402.48 is a hexane medium density polyethylene blown film grade for applications requiring high stiffness. It can also be used in cast films. Films produced from the resin e.. |
|||
Dart Drop Test | <= 50.0 g | <= 0.110 lb | ASTM D1709A |
ExxonMobil LLDPE LL 3402.48 Cast Linear Low Density Polyethylene Resin Product Description: LL 3402.48 is a hexane medium density polyethylene cast film grade for applications requiring high stiffness. It can also be used in blown films. Films produced from this resin .. |
|||
Dart Drop Test | <= 50.0 g | <= 0.110 lb | ASTM D1709A |
ExxonMobil LLDPE LL 3404.48 Linear Low Density Polyethylene Resin Product Description: LL 3404.48 is a hexane medium density polyethylene cast film grade for applications requiring high strength and high stiffness. Films produced from this resin exhibit good tensi.. |
|||
Dart Drop Test | 50.0 g | 0.110 lb | ASTM D1790 |
ExxonMobil HD 7925.30 Barrier Film Resin Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements.A.. |
|||
Dart Drop Test | <= 50.0 g | <= 0.110 lb | g/F50; ASTM D1709 |
Braskem EB853 Cast Film Extrusion Low Density Polyethylene LLDPE and HDPE blends.Information provided by Braskem. |
|||
Dart Drop Test | 50.0 g | 0.110 lb | ASTM D1709 |
Huntsman Rexell® M3107 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, .. |
|||
Dart Drop Test | 50.0 g | 0.110 lb | ASTM D1709 |
Huntsman PE1059 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down and good processability.Applications: Film extrusion: non-abrasive packaging applications.FDA Notes: Conforms to FDA regulation 21 CFR 177.. |
|||
Dart Drop Test | 50.0 g | 0.110 lb | ASTM D1709 |
Huntsman PE1076 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (.. |
|||
Dart Drop Test | 50.0 g | 0.110 lb | ASTM D1709 |
Huntsman PE1078 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (.. |
|||
Dart Drop Test | 50.0 g | 0.110 lb | ASTM D1709 |
Huntsman PE8020 Specialty Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1.. |