Mechanical Properties Metric English Comments
Dart Drop Test 210 g
0.463 lb
F50; ISO 7765-1
Polimeri Europa Clearflex® CL D0 Very Low Density Polyethylene
Clearflex CL D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).This resin is produced with a proprietary technology. Stretch films manufactured..
Dart Drop Test >= 210 g
>= 0.463 lb
ASTM D1709
NIZHNEKAMSKNEFTEKHIM PE 5117N (18601) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Dart Drop Test >= 210 g
>= 0.463 lb
ASTM D1709
NIZHNEKAMSKNEFTEKHIM PE 5118N (18601) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Dart Drop Test >= 210 g
>= 0.463 lb
ASTM D1709
NIZHNEKAMSKNEFTEKHIM PE 5118P (18602) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Dart Drop Test 210 g
0.463 lb
(method A); ASTM D1709
Petroquimica Triunfo Trithene® TS 7001 LDPE - Heavy Duty Low Friction Film
The Trithene TS 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and low coefficient of fricti..
Dart Drop Test 210 g
0.463 lb
(method A); ASTM D1709
Petroquimica Triunfo Trithene® TX 7001 LDPE - High Molecular Weight
The Trithene TX 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and environmental stress crac..
Dart Drop Test 210 g
0.463 lb
ASTM D1709-98
Ipiranga Petrochem LB 0117 LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Dart Drop Test 210 g
0.463 lb
ASTM D1709
Iran Petrochemical (PCC) EX 4HS HM 9455 F1 High Density Polyethylene
EX 4HS is a high density polyethylene with 1-Butene as co monomer. It has high rigidity, low gel level, high drawdown, very high stiffness and good tenacity.Applications: film extrusion, blending ..
Dart Drop Test 210 g
0.463 lb
ASTM D1709
Formosa Plastics Formolene® E924 Film HDPE
High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E924 is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristics..
Dart Drop Test 210 g
0.463 lb
ASTM D1709A
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin
Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Dart Drop Test 210 g
0.463 lb
ASTM D1709A
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin
Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Dart Drop Test 210 g
0.463 lb
ASTM-D1709
Braskem GM9450F HDPE Blown Film Extrusion Polyethylene
HDPE GM9450F is a high-density polyethylene developed for the high molecular weight film extrusion segment produced with bimodal technology. The film produced from this resin has high tenacity and e..
Dart Drop Test 210 g
0.463 lb
ASTM D1709A
ExxonMobil Enable™ 20-05CB Metallocene Polyethylene Resin
Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Dart Drop Test 210 g
0.463 lb
ASTM D1709
Formosa Plastics Formolene® E924F Film HDPE
High Density Polyethylene High Molecular Weight Bi-Modal Resin for Film Applications Formolene® E924F is a “low gel” high molecular weight grade of HDPE designed for high dart impact strength and..