Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 140 g | 0.309 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FH 20 Low Density Polyethylene - Blown Film Extrusion Riblene FH 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Dart Drop Test | 140 g | 0.309 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trithene® CX 7020 LDPE - Cast Film The Trithene® CX 7020 resin is a low-density polyethylene (LDPE) with medium molecular weight, excellent processability, and low gel content. Those features allow a production of thin and highly un.. |
|||
Dart Drop Test | 140 g | 0.309 lb | 26 in; ASTM D1709 |
Chevron Phillips mPact™ D352 m-LLDPE Linear Low Density Polyethylene
(discontinued **) Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin provides increased modulus over most LLDPE's while retaining excellent clarity and good toughness. Applications: Industr.. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709 |
ExxonMobil Exceed™ 3518 GA Premium Cast Film Resin
(discontinued **) Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Dart Drop Test | 140 g | 0.309 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA340141 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
Dart Drop Test | 140 g | 0.309 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA340163 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
Dart Drop Test | 140 g | 0.309 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA340013 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
Dart Drop Test | 140 g | 0.309 lb | ISO 7765-1 |
Borealis FA5223 Low Density Polyethylene FA5223 is a Low Density Polyethylene for Film Extrusion. Contains antioxidant and antiblock additive. This grade is developed to give strong film for medium duty applications. Applications FA5223.. |
|||
Dart Drop Test | 140 g @Thickness 0.0400 mm |
0.309 lb @Thickness 0.00157 in |
ISO 7765-1 |
Borealis FA5224 Low Density Polyethylene FA5224 is a Low Density Polyethylene for Film Extrusion. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed to give strong film for medium duty applications. Appl.. |
|||
Dart Drop Test | 140 g @Thickness 0.0400 mm |
0.309 lb @Thickness 0.00157 in |
ISO 7765-1 |
Borealis FG5190 Linear Low Density Polyethylene FG5190 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes Antioxidant. The grade is developed for medium and heavy duty bags, bags and bin liners, dual stretch films, and film.. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709A |
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709 |
ExxonMobil Exceed™ 1327HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1327HA resin have excellent tensile, impact strength and puncture. These superior strength prope.. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709 |
ExxonMobil Exceed™ 1327KD Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327KD is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327KD is fully formula.. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709 |
ExxonMobil Exceed™ 4518PA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 4581PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 4581PA have outstanding tensile properties and impact and puncture toughness. These superior prope.. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709 |
ExxonMobil LD 103.59 Industrial Film Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709 |
ExxonMobil LD 144.50 Packaging Film Resin Film made from LD 144.50 offers improved impact strength and heat sealability compared to homopolymer clarity film resins. Typically applications include food packaging, frozen food packaging, and .. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709 |
ExxonMobil LD 313.NF Blown Film Resin LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr.. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709A |
ExxonMobil LDPE LD 103.09 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709A |
ExxonMobil LDPE LD 103.59 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709A |
ExxonMobil LDPE LD 159AC Low Density Polyethylene Resin Product Description: LD 159AC is an LDPE grade, which offers good draw down combined with good mechanical strength. Availability: Africa & Middle East and Europe Additive: Antiblock: 450 ppmSlip: 5.. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709A |
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709A |
ExxonMobil LDPE LD 363BW Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709A |
ExxonMobil LLDPE LL 3001.63 Linear Low Density Polyethylene Resin Product Description: LL 3001.36 is a hexane copolymer LLDPE film resin. Films made from this resin have outstanding tensile and toughness properties. Superior strength properties, along with excell.. |
|||
Dart Drop Test | 140 g | 0.309 lb | |
Dow LDPE 683I Low Density Polyethylene, Film Grade DOW LDPE 683I resin is a general purpose resin with low levels of antiblock additive used for frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.. |
|||
Dart Drop Test | 140 g | 0.309 lb | gF/50%f; ASTM D1709 |
Braskem EB861 Blown Film Extrusion Low Density Polyethylene Medium-resistance films for general use; Mulching films; Shrink films; Coextrusion.Information provided by Braskem. |
|||
Dart Drop Test | 140 g | 0.309 lb | gF/50%f; ASTM D1709 |
Braskem EB861/51 Blown Film Extrusion Low Density Polyethylene Film for general use; Shrink films; Coextrusion.Additives: Antiblock, DInformation provided by Braskem. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709 |
Huntsman Rexell® L3103 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent optics and sealability with good toughnessApplications: Stretch wrap and coextruded film for general packaging.FD.. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709 |
ExxonMobil Exceed™ 3518 CB Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709 |
ExxonMobil Exceed™ 3518 PA Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Dart Drop Test | 140 g | 0.309 lb | ASTM D1709 |
ExxonMobil Exceed™ 4518CB Metallocene Polyethylene Resin Product Description: Exceed 4518 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 4518 have outstanding tensile properties and impact and puncture toughness. These superior p.. |