Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 100 g | 0.221 lb | F50; ISO 7765-1 |
Polimeri Europa Eraclene® FA 706 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 706 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Films manufactured with Eraclene FA 706 show good processability t.. |
|||
Dart Drop Test | >= 100 g | >= 0.221 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 4118N (18401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Chevron Phillips mPact™ D353 m-MDPE Linear Low Density Polyethylene
(discontinued **) Low Density PolyethyleneCustomer Benefits: This metallocene medium density PE for cast film applications offers greater tensile modulus than LLDPE while retaining excellent optical properties.Data p.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Formosa Plastics Formolene® L62608PE Film (Hexene Grade) LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
ExxonMobil LD 135.09 Blown Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. Applications include food packaging, light to medium duty bags, and textile packaging.Information provided by ExxonMobil Chemical |
|||
Dart Drop Test | 100 g | 0.221 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Dart Drop Test | 100 g | 0.221 lb | |
DuPont™ Sclairfilm® LWS-1 LMDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
LyondellBasell Montell 12C01G2 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
LyondellBasell Montell 12C01G5 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene 09X02 is a high performance LLDPE (HP-LLDPE) cast film grade combines ease of processing with low gels and good film strength. Its excellent stretchability makes this grade particularly suited for s.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Iran Petrochemical (PCC) LF0200 Low Density Polyethylene LF0200 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. LF0200 contains antioxidant.Applications: genera.. |
|||
Dart Drop Test | 100 g @Thickness 0.0254 mm |
0.221 lb @Thickness 0.00100 in |
High Stalk Extrusion - 6:1 FLH/D ratio and 4:1 BUR; ASTM D1709A |
Total HL 428 HDPE Film Grade Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
ExxonMobil LDPE LD 105.30 Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Film; 50.8 microns; ASTM D1709B |
Dow DX5E66 Polypropylene Homopolymer Resin OverviewConsistent processabilityVery high cleanlinessGood optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c)1.1a, EU-Directive 2002/72/EC, Canadian HPFB No ObjectionDX5E66 Developmental P.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7065 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709A |
ExxonMobil Escorene™ LD 706.15 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for coextruded cast film applications.Availability: Latin America, North America and South Ame.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7065 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7094 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |
|||
Dart Drop Test | <= 100 g | <= 0.221 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-7002 NT 7 is an ethylene-hexene-1 copolymer, design.. |
|||
Dart Drop Test | 100 g | 0.221 lb | g/F50; ASTM D1709 |
Braskem Green PE SLL218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL218 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for cast film extrusion. Films obtained with this product show a good processing performance balanced with .. |
|||
Dart Drop Test | 100 g | 0.221 lb | ASTM D1709 |
Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Stretch film; shrink film; "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem |
|||
Dart Drop Test | 100 g | 0.221 lb | gF/50%f; ASTM D1709 |
Braskem BF0323/12HC Blown Film Extrusion Low Density Polyethylene Shrink films; Automatic packaging of liquid products (FFS).Additives: Antiblock, DInformation provided by Braskem. |
|||
Dart Drop Test | 100 g | 0.221 lb | |
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Dart Drop Test | 100 g | 0.221 lb | gF/50%f; ASTM D1709 |
Braskem BF0323HC Blown Film Extrusion Low Density Polyethylene Heavy-duty bags; Agriculture, Coextruded and shrink films for pallets.Information provided by Braskem. |
|||
Dart Drop Test | 100 g | 0.221 lb | gF/50%f; ASTM D1709 |
Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol process technology. It shows excellent optical properties associated with good balance of mechanical properties, processing.. |