Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | >= 4.72 g/micron | >= 120 g/mil | ASTM D1922 |
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Elmendorf Tear Strength, MD | >= 4.72 g/micron | >= 120 g/mil | ASTM D1922 |
NIZHNEKAMSKNEFTEKHIM PE 4121N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Elmendorf Tear Strength, MD | 4.72 g/micron | 120 g/mil | ASTM D1922 |
ExxonMobil LL 1002.32 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength, MD | 4.72 g/micron | 120 g/mil | ASTM D1922 |
ExxonMobil LL 1002x74 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength, MD | 4.72 g/micron | 120 g/mil | ASTM D1922 |
ExxonMobil LL 1002x79 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength, MD | 4.72 g/micron | 120 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-104 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer packaging film resin with excellent clarity and good stiffness. It is excellent either blown film or chill roll casting equipment. I.. |
|||
Elmendorf Tear Strength, MD | >= 4.72 g/micron | >= 120 g/mil | ASTM D1922 |
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Elmendorf Tear Strength, MD | >= 4.72 g/micron | >= 120 g/mil | ASTM D1922 |
NIZHNEKAMSKNEFTEKHIM PE 4122N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Elmendorf Tear Strength, MD | 4.72 g/micron | 120 g/mil | ASTM D1922 |
ExxonMobil Escorene® CR-5810 EVA Resin, for High Cling Stretch Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A tackified Ethylene Vinyl Acetate resin for blown or cast stretch film.Applications: Packing films (cling). Data for film properties below based o.. |
|||
Elmendorf Tear Strength, MD | 4.72 g/micron | 120 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-318 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-318 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Elmendorf Tear Strength, MD | 4.72 g/micron | 120 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-319 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-319 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Elmendorf Tear Strength, MD | 4.72 g/micron | 120 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-336 EVA Film Resin, Clarity, Very High Drawdown
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer blown film resin capable of very high drawdown with excellent clarity.Applications: Very thin heat seal layers; Light.. |
|||
Elmendorf Tear Strength, MD | 4.72 g/micron | 120 g/mil | ASTM D1922 |
SIDPEC EGYPTENE® LL 0220 AA LLDPE Film Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Elmendorf Tear Strength, MD | 4.72 g/micron | 120 g/mil | ASTM D1922 |
SIDPEC EGYPTENE® LL 0220 KJ LLDPE Film Applications: Light and medium duty film.Film properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor of Sidi Ke.. |
|||
Elmendorf Tear Strength, MD | 4.72 g/micron | 120 g/mil | 50 µm (2 mil) film; ASTM D1922 |
DuPont Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Elmendorf Tear Strength, MD | 4.72 g/micron | 120 g/mil | ASTM D1922 |
ExxonMobil LL 1002.09 Blown Film Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Elmendorf Tear Strength, MD | 4.72 g/micron | 120 g/mil | ASTM D1922 |
ExxonMobil LL 1002x75 Blown Film Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |