Polymer Property : Elmendorf Tear Strength, MD = 6.30 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD >= 6.30 g/micron
>= 160 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, MD >= 6.30 g/micron
>= 160 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 4116N (16401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, MD 6.30 g/micron
160 g/mil
ASTM D1922
NOVA Chemicals Novapol® LA-0424-A LDPE Foam Resin
Good stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film extr..
Elmendorf Tear Strength, MD 6.30 g/micron
160 g/mil
ASTM D1922
NOVA Chemicals Novapol® TF-Y826-CP Hexene LLDPE Film Resin
Film Properties. Features: Good stiffness, intended for narrow die gaps, high strength and toughness.Applications: Industrial bags, industrial packaging.Data provided by the manufacturer.
Elmendorf Tear Strength, MD 6.30 g/micron
160 g/mil
ASTM D1922
ExxonMobil Exceed™ 1327CA Blown Film Resin  (discontinued **)
Exceed 1327CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1327CA resin have outstanding tensile, impact strength and puncture. These superi..
Elmendorf Tear Strength, MD 6.30 g/micron
160 g/mil
ASTM D1922
NOVA Chemicals Novapol® TF-Y826-D Hexene LLDPE Film Resin
Film Properties. Features: High strength and toughness, excellent puncture resistance, good stiffness and machinability.Applications: Premium trash bags, bags-on-roll.Data provided by the manufactu..
Elmendorf Tear Strength, MD 6.30 g/micron
160 g/mil
ASTM D1922
Formosa Plastics Formolene® L42009A Film (Butene Grade) LLDPE
Butene Copolymer (High Antiblock)Applications: Blown file for either blending or extrusionBlown file for either blending or extrusionMeets all requirements of the U.S. Food and Drug Administration a..
Elmendorf Tear Strength, MD 6.30 g/micron
160 g/mil
ASTM D1922
Formosa Plastics Formolene® L42009M Film (Butene Grade) LLDPE
Butene Copolymer (High slip and antiblock)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of poly..
Elmendorf Tear Strength, MD 6.30 g/micron
160 g/mil
ASTM D1922
ExxonMobil LD 313.NF Blown Film Resin
LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr..
Elmendorf Tear Strength, MD 6.30 g/micron
160 g/mil
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.
Elmendorf Tear Strength, MD 6.30 - 27.0 g/micron
160 - 686 g/mil
Average value: 11.1 g/micron Grade Count:18
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is ..
Elmendorf Tear Strength, MD 6.30 g/micron
160 g/mil
ASTM D1922
NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Good stiffness and machinability, intended for narrow die gaps, high strength and toughness.Applications: Grocery sacks, boutique bags, frozen food packaging.Data provide..