Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 1.20 J/cm² @Temperature -40.0 °C |
5.71 ft-lb/in² @Temperature -40.0 °F |
cond; ISO 180/1A |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Izod Impact Resistance | 1.20 J/cm² @Temperature -40.0 °C |
5.71 ft-lb/in² @Temperature -40.0 °F |
dry; ISO 180/1A |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Izod Impact Resistance | 1.20 J/cm² @Temperature -40.0 °C |
5.71 ft-lb/in² @Temperature -40.0 °F |
cond; ISO 180/1A |
DSM Stanyl® TS250F8 PA46-GF40 FR 40% Glass Reinforced, Flame Retardant, Heat Stabilized |
|||
Izod Impact Resistance | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 180/1A |
DSM Stanyl® TS250F8 PA46-GF40 FR 40% Glass Reinforced, Flame Retardant, Heat Stabilized |
|||
Izod Impact Resistance | 1.20 J/cm² @Temperature -40.0 °C |
5.71 ft-lb/in² @Temperature -40.0 °F |
dry; ISO 180/1A |
DSM Stanyl® TS250F8 PA46-GF40 FR 40% Glass Reinforced, Flame Retardant, Heat Stabilized |
|||
Izod Impact Resistance | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 180/1A |
DSM Stanyl® TW241B3 PA46-CF15 15% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Izod Impact Resistance | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 180/1A |
DSM Stanyl® TW271B3 (PA46+PTFE)-CF15 15% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Izod Impact Resistance | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 180/1A |
DSM Stanyl® TS200F6 PA46-GF30 30% Glass Reinforced |