Mechanical Properties Metric English Comments
Shear Modulus 3.50 GPa
508 ksi
Calculated
Premix Premi-Glas® 1201-15 Polyester SMC
Premi-Glas® 1201-15 is a 15% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS..
Shear Modulus 3.50 GPa
508 ksi
Calculated
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Shear Modulus 3.50 GPa
508 ksi
Calculated
Premix Premi-Glas® 2203-15 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Shear Modulus 3.50 GPa
508 ksi
Calculated
Premix Premi-Glas® 2203-15 CR-SX-HT Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2203-15 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL..
Shear Modulus 3.50 GPa
508 ksi
Calculated
Premix Premi-Glas® 2204-15 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2204-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Shear Modulus 3.50 GPa
508 ksi
Calculated
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Shear Modulus 3.50 GPa
508 ksi
Calculated
Premix Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2206-15 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
Shear Modulus 3.50 GPa
508 ksi
Calculated
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
Shear Modulus 3.50 GPa
508 ksi
Calculated
Premix Premi-Glas® 3200-15 Fiberglass Reinforced SMC
Description: Premi-Glas® 3200-15 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di..
Shear Modulus 3.50 GPa
508 ksi
Calculated
Premix Premi-Ject® 1102H Fiberglass Reinforced Thermoset BMC
Premi-Ject® 1102H is a fiberglass reinforced thermoset bulk molding compound for coil encapsulation applications.Key features and benefits are:Designed with unique flow properties to encapsulate co..
Shear Modulus 3.50 GPa
508 ksi
calculated
BASF Capron® HPN 9333G Impact Modified, 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9333G is a 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface a..
Shear Modulus 3.50 GPa
508 ksi
calculated
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with..
Shear Modulus 3.50 GPa
508 ksi
in plane
Menzolit Menzolit® BMC 2310 Unsaturated Polyester UP
BMC 2310 is a chemically resistant grade reinforced with special fibres. Being completely glass-free (no glass fibre reinforcement) it is specifically recommended for the manufacture of high voltage..
Shear Modulus 3.50 GPa
508 ksi
in plane
Menzolit Menzolit® SMC 0200 Unsaturated Polyester UP
SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands ..
Shear Modulus 3.50 GPa
508 ksi
in plane
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP
SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel..
Shear Modulus 3.50 GPa
508 ksi
in plane
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP
SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is ..
Shear Modulus 3.50 GPa
508 ksi
In-Plane, RT, Dry; EN6031
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber
Information provided by HexCel