Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 4.15 - 4.47 GPa | 602 - 648 ksi | Calculated |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Shear Modulus | 4.15 GPa | 602 ksi | Calculated |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl.. |
|||
Shear Modulus | 4.15 - 4.47 GPa | 602 - 648 ksi | Calculated |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
Shear Modulus | 4.15 - 5.18 GPa | 602 - 751 ksi | Average value: 4.58 GPa Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
Shear Modulus | 4.15 - 4.36 GPa | 602 - 632 ksi | Calculated |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |