Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.Key features and benefits.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 1205 Glass Reinforced SMC Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 2200-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2200-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Pigmentable for molded-in c.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 2203-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Excellent stiffness to weight rat.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 2203-20 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 2204-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2204-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Good dimensional stability, inclu.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 2205-20 CRSX Polyester SMC Premi-Glas® 2205-20 CR-SX is a 20% fiberglass reinforced Sheet Molding Compound formulated for condensate pan applications requiring chemical resistance, heat resistance, dimensional stability, we.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 3200-22 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-22 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Premix Premi-Glas® 3404 33% Glass Reinforced SMC Description: Premi-Glas® 3404 is a glass reinforced thermoset sheet molding compound designed for mass transit and high strength flame retardant applications where low smoke and flame are required... |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Plenco 7466 Phenolic, Nodular, Injection Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07466 is a flock cotton and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. UL recognized under component file E406.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | in plane |
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP SMC 0600 is a specially formulated SMC for reduced moulding pressure (< 30 bar). The glass level has been selected to combine good mouldability with strength and stiffness. Even without a specific f.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | in plane |
Menzolit Menzolit® SMC 0650 Unsaturated Polyester UP SMC 0650 Low pressure SMC for large panels when moulding force becomes critical. Specific moulding pressure < 20 bar. A Special molding procedure is necessary.Information Provided by Menzolit |
|||
Shear Modulus | 3.80 GPa | 551 ksi | in plane |
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | Calculated |
Plenco 4466 Phenolic, Granular, Transfer Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Shear Modulus | 3.80 GPa | 551 ksi | calculated |
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he.. |