Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.52 GPa | 801 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-NY-027-SS-BLK-F Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 5.52 GPa | 801 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID® 66 GF 15 002 PA66 reinforced with glass fiber PA66 for injection molding, reinforced with 15 % glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools,.. |
|||
Tensile Modulus | 5.52 GPa | 801 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PF-20GF/000 Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 5.52 GPa | 801 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PK-10GF/000 Polyetheretherketone (PEEK) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 5.52 GPa | 801 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ 81510 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 5.52 GPa | 801 ksi | ASTM D638 |
Solvay Specialty Polymers PrimoSpire® PR-250 Polyphenylene, Self-Reinforced (SRP) PrimoSpire® PR-250 resin is an injection molding grade of self-reinforced polyphenylene (SRP). PrimoSpire® SRP is an ultra-high performance amorphous, melt-processable polymer. The unique prop.. |
|||
Tensile Modulus | 5.52 GPa | 801 ksi | 1 mm/min |
Arkema Group Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,GF23Rigid grade with glass fiber filler (23%) for injection molding. Available colors: black and natural. Reinforced light and heat stabilizing agent. Mold-rele.. |
|||
Tensile Modulus | 5.52 GPa | 801 ksi | ASTM Test |
BASF Ultradur B 4300 G3 15% Glass Filled PBT Ultradur B 4300 G3 is an easy flowing injection molding PBT with 15% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Tensile Modulus | 5.52 GPa | 801 ksi | |
Reliance Industries Polypropylene - 40% Glass filled Information provided by Reliance Industries |
|||
Tensile Modulus | 5.52 GPa | 801 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1040 PP SABIC® PPcompound 15T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound, suitable for injection molding applications. The IMDS ID is 16487994 |