Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.460 GPa @Temperature 120 °C |
66.7 ksi @Temperature 248 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 0.460 GPa | 66.7 ksi | 1 mm/min |
Arkema Group Rilsan® 8020 Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11/xx,E,16-003Transparent and flexible copolymer for tubes extrusion. Additive free.Good flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |
|||
Tensile Modulus | 0.460 GPa | 66.7 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8254 HS BK-102 PA6 (Conditioned) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
Tensile Modulus | 0.460 GPa | 66.7 ksi | 1 mm/min |
Arkema Group Orgalloy® LT 5050 Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good .. |
|||
Tensile Modulus | 0.460 GPa | 66.7 ksi | 1 mm/min |
Arkema Group Orgalloy® LT 5050ES Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good .. |
|||
Tensile Modulus | 0.460 GPa | 66.7 ksi | 1 mm/min |
Arkema Group Orgalloy® LT 5050T Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good .. |