Arkema Group Rilsan® 8020 Nylon 11, Flexible Tubing Grade (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Flexible Tubing Grade
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® 8020 Nylon 11, Flexible Tubing Grade (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Designation ISO 1874-PA11/xx,E,16-003Transparent and flexible copolymer for tubes extrusion. Additive free.Good flexibility. Very good transparency. High chemical resistance.USP XXIII class VI approval. Food contact approval EEC directive N 90/128. Example applications: Beer tubing, catheters.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
Water Absorption 1.5 %
1.5 %
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 235 °C
14 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 26 %
26 %
50 mm/min
Tensile Modulus 0.460 GPa
66.7 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched NB
NB
0.910 J/cm²

@Temperature -30.0 °C
4.33 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 171 °C
340 °F
10°C/min
Glass Transition Temp, Tg 34.0 °C
93.2 °F
10°C/min
Flammability, UL94 V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.