Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.70 GPa | 392 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 FRC 2 LS Polyamide 6, Halogen Free Flame Retardant, Light Stabilization FeaturesLongterm external use is possible because of the material stabilization with the light stabilizers on the HALS basis. Meets the flammability in accordance with the norm DIN 4102 - B1. PA 6.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® EFX830ME PC Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering metallic / sparkle look with minimal flow line visibilityThis data was supplied by SABIC-.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527 |
Nilit FRIANYL A63 S10 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527 |
Nilit RECONYL B Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1/-2 |
Lanxess Pocan® DP 1105 000000 PBT PBT, non-reinforced, injection molding, extrusion, improved flowability |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific) NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1 |
Sax Polymers SAXLAC 207 Acrylonitrile Butadiene Styrene Saxalac 207 is a high heat ABS, characterized by high impact strength and high stiffness.Mechanical property data tested at 50% RH.Information provided by SAX Polymers |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527-1,-2 |
Covestro Bayblend® FR3006 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 MR 309 HWCP 30% Mineral Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT3Z LF black 9564 PA* Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT produc.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSS PA666 Product description: Grilon TSS is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS has the following important properties: Excellent flow behaviorHi.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min |
Arkema Group Lucalor® PEY 436 CPVC, Pipe Grade LUCALOR PEY 436 is a chlorinated polyvinyl chloride compound (CPVC) developed for the extrusion of pipes for hot water supply and distribution systems.ISO data provided by the manufacturer, Arkema. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1/-2 |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1/-2 |
BASF Ultraform® S2320 003 POM Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1/-2 |
DSM Arnite® T06 202 /A PBT Medium Viscosity, Injection Molding |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1, 2 |
Polyplastics Duracon® M90-71 Acetal Co-polymer (POM), Heat resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | |
Covestro Bayblend® FR 2010 Polycarbonate/ABS Blend
(discontinued **) Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1 |
Sax Polymers SAXATEC 4120 Acrylonitrile Styrene Acrylate SAXATEC 4120 is a easy lowing, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX Polym.. |