Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 3.63 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.0250 GPa
3.63 ksi
1 mm/min; ASTM D638 - ISO 527-2
DuPont Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer
Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill..
Tensile Modulus 0.0250 GPa
3.63 ksi
1 mm/min; ASTM D638 - ISO 527-2
DuPont Elvaloy® 3427 AC Ethylene and 27% Butyl Acrylate Copolymer
Elvaloy® 3427 AC can be used for coextrusion and compounding. It can also be used in extrusion coating. Elvaloy® 3427 AC is very soft and flexible, and has good adhesion to various polymers. It..
Tensile Modulus 0.0250 GPa
3.63 ksi
ISO 527-1/-2
DSM Arnitel® EL250 TPC-ET
Injection Molding
Tensile Modulus 0.0250 GPa
3.63 ksi
ISO 527-1/-2
DuPont Performance Polymers Hytrel® G3548 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
35 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers