Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527 |
Premix Thermoplastics PRE-ELEC® 12-033
(discontinued **) PRE-ELEC 12-033 is a conductive thermoplastic compound based on a polyacetal copolymer with 30% carbon fiber. PRE-ELEC 12-033 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA)
(Unverified Data**) Ixef 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1025/9.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA)
(Unverified Data**) Ixef 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance. - Natural: Ixef.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, DRY Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Omnix® 4050 Polyamide, High Performance (HPPA) (Dry) Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used .. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Omnix® 9050 Polyamide, High Performance (HPPA), 50% Glass Fiber Omnix® 9050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture ab.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 1SVX-65H black 9288 PA1010-GF65 Product Description: Grilamid 1SVX-65H black is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources Exc.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 1SVX-65H nat PA1010-GF65 Product Description: Grilamid 1SVX-65H natural is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-1/-2 |
DSM Stanyl® TE250F9 (DAM) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5H EF black 9915 PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50 Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVS-5H nat PA*-GF50 Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LVX-65H SST nat PA12-GF65 Product description: Grilamid LVX-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following pro.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR50 BK009 MX01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, improved impact, natural Information provided by Eurotec® |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR50 NL RM PA6.6, 50% glass fiber reinforced, MoS2 modified, natural Information provided by Eurotec® |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50 Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac.. |
|||
Tensile Modulus | 17.0 GPa @Temperature 80.0 °C |
2470 ksi @Temperature 176 °F |
|
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
CENTROPLAST CENTROMID 6.6 CF 20 Polyamide 6.6 carbon fiber This material has very high strength and a high operating temperature. It can be used for precision components, drive parts and housings.Information provided by CENTROPLAST Engineering Plastics GMB.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVX-5 H nat PA*-GF50 Product description: Grivory GVX-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | |
LATI Latiohm 66-04 PD01 G/25-V0CT1 PA66, 25% Glass Fiber Reinforced, Flame Retardant Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific;.. |