Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.69 GPa @Thickness 3.20 mm |
245 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical HI100H ABS, High Impact, High Toughness Feature: Injection Molding, High Impact, High ToughnessApplication: Helmet, Pipe & Fittings)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 1-3000 N DEL Polypropylene Homopolymer INNOPOL® CS 1-3000 N DEL is developed for producing injection molded automotive components.All information provided by INNO-COMP. |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Asia Pacific) Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Europe-Africa-Middle East) Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® X6800BM PBT Blow moldable, impact modifed XENOYThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X6800BM PBT (Asia Pacific) Blow moldable, impact modifed XENOY |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X8303 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized. For In Mold Decoration /Labeling. |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | ASTM D 638 |
Styrolution PS 5410 HIPS Good printabilityGood environmental stress crack resistanceLow GelsTrims CleanlyLow Gloss (matte finish)Information provided by Styrolution |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | ISO527-2/1 |
ExxonMobil AP3N Polypropylene Impact Copolymer Product Description: A medium impact copolymer resin designed for appliance applications requiring good stiffness and fast cycle time.Availability: Asia Pacific Features:Fast Molding CycleHigh Glos.. |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | 1 mm/min |
Arkema Group Rilsan® AESN TL Nylon 12, Flexible Tubing Grade (Dry) Designation ISO 1874-PA12,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. Good chemical resistance. Very good ability .. |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | conditioned 15 days, 23°C - 50 % R.H.; ISO 527 |
Arkema Group Rilsan® Clear G380 Renew Polyamide Rilsan® Clear G830 Rnew is a high performance transparent polyamide partially based on renewable resources. This grade has been specially designed for injection molding applications, ideally suited.. |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | |
Ineos ABS Triax® 1180 ABS + Polyamide Blend (DAM)
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business r.. |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X6800BM PBT (Europe-Africa-Middle East) Blow moldable, impact modifed XENOY |
|||
Tensile Modulus | 1.69 GPa | 245 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon MDM40 PP LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region. |